Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Eastar™ DN004 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Eastar™ DN004:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Eastar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文

Eastar™ copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. Eastar™ DN004 copolyesters are the toughest materials for the

cosmetics and personal care packaging applications. It's very shatter resistant and offers excellent chemical resistance. DN004 contains a mold release.

Processing/Physical Characteristics単位テスト基準
ASTM数据
成形収縮率., 平行 0.0035 mm/mm ASTM D 955
機械的特性単位テスト基準
ISO データ
降伏応力 46 MPa ISO 527
降伏ひずみ 4.4 % ISO 527
破壊応力 47 MPa ISO 527
破壊ひずみ 230 % ISO 527
曲げ弾性率, 23°C 1800 MPa ISO 178
ノッチ付きIzod衝撃強さ, +23°C 125 kJ/m² ISO 180/1A
ノッチ付きIzod衝撃強さ 7.4 kJ/m² ISO 180/1A
温度 -40 °C -
パンクチャー衝撃エネルギー, +23゚C 14 J ISO 6603-2
ASTM数据
引張弾性率 1800 MPa ASTM D 638
降伏応力 45 MPa ASTM D 638
破壊応力 52 MPa ASTM D 638
降伏点伸び 5 % ASTM D 638
破断伸び 330 % ASTM D 638
曲げ弾性率 1800 MPa ASTM D 790
ロックウェル硬度 105 - ASTM D 785
ノッチ付きIzod衝撃強さ, 1/8 in N J/m ASTM D 256
ノッチ付きIzod衝撃強さ, Low-Temperature 64.1 J/m ASTM D 256
温度 -40 °C -
アイゾット衝撃試験, 1/8 in N J/m ASTM D 256
熱的特性単位テスト基準
ISO データ
荷重たわみ温度, 1.80 MPa 65 °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 74 °C ISO 75-1/-2
ビカット軟化温度, A 88 °C ISO 306
ビカット軟化温度, B 79 °C ISO 306
1.5mm厚さでの燃焼性 HB class IEC 60695-11-10
試験片の厚さ 1.6 mm -
厚さhでの燃焼性 HB class IEC 60695-11-10
試験片の厚さ 3.2 mm -
ASTM数据
UL94 燃焼性 HB - UL 94
追加試験片の厚さ 1.6 mm -
DTUL @ 66 psi 74 °C ASTM D 648
DTUL @ 264 psi 64 °C ASTM D 648
ビカット軟化温度 88 °C ASTM D 1525
熱伝導率, ソリッド 0.0274 W/(m K) ASTM C 177
電気的特性.単位テスト基準
ASTM数据
耐電圧, 短い時間 16.3 kV/mm ASTM D 149
誘電正接, 1 MHz 0.013 - ASTM D 150
比誘電率, 1 MHz 2.8 - ASTM D 150
表面抵抗率 1E16 Ohm ASTM D 257
体積抵抗率 1E15 Ohm*cm ASTM D 257
耐アーク 138 s ASTM D 495
光学特性単位テスト基準
ASTM数据
ヘイズ 1 % ASTM D 1003
視感透過率 89 % ASTM D 1003
その他の特性.単位テスト基準
密度. 1230 kg/m³ ISO 1183
吸水率, 24hr 0.13 % ASTM D 570
密度 1230 kg/m³ ASTM D 792
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 71 °C -
Pre-drying - Time 6 h -
樹脂温度 250 - 270 °C -
金型温度 15 - 40 °C -
特殊な特性
成形加工法.
射出成形.
納入形状.
ナチュラルカラー
添加剤.
離型剤.
特殊な特性.
高耐衝撃及び耐衝撃改良.
な特性
Color Stability, Copolymer
耐薬品性
General Chemical Resistance, Solvent Resistance, Radiation Resistance
Certifications
Food contact
アプリケーション
医療の, パッケージング, スポーツ用品
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ., 近東/アフリカ
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.