Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of ecovio® M2351 - (PBAT+PLA) - BASF

Material Data Center offers the following functions for ecovio® M2351:
unit conversion, PDF datasheet print, comparison with other plastics, application examples, CAE Interfaces

Check here, which other Ecovio datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトボリュームレイト, MVR 8 cm³/10min ISO 1133
温度 190 °C -
荷重 5 kg -
その他の特性.単位テスト基準
密度. 1390 kg/m³ ISO 1183
Bulk density 800 kg/m³ -
機械的特性(ィルム)単位テスト基準
ISO データ
引張弾性率, 平行 260 MPa ISO 527-3
引張弾性率, 直角 130 MPa ISO 527-3
最大応力, 平行 25 MPa ISO 527-3
最大応力, 平行 20 MPa ISO 527-3
最大ひずみ, 平行 180 % ISO 527-3
最大ひずみ, 直角 380 % ISO 527-3
押出成形のタイプ. blown - -
試験片の厚さ. 0.012 mm -
特殊な特性
成形加工法.
Blown Film Extrusion, フィルム押出成形.
納入形状.
ペレット.
添加剤.
滑剤., ブロッキング防止剤.
な特性
Melt Strength, Thermal Stability
Certifications
Contains renewable resources, Biodegradable, Food contact, 堆肥化可能 ISO 13432 (プロデューサー), 堆肥化可能 ASTM D6400 (プロデューサー), 堆肥化可能 ISO 13432 (証明書), 堆肥化可能 ASTM D6400 (証明書)
領域別の利用可能性
ヨーロッパ.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com