Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of ECOZEN® HF502 - Copolyester - SK Chemicals

Material Data Center offers the following functions for ECOZEN® HF502:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Ecozen datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
ECOZEN, conceived and developed by SK Chemicals is a bio-based, heat-resistant, and transparent bio-copolyester.
Processing/Physical Characteristics単位テスト基準
ASTM数据
成形収縮率., 平行 0.0035 mm/mm ASTM D 955
機械的特性単位テスト基準
ISO データ
降伏応力 59 MPa ISO 527
降伏ひずみ 4.8 % ISO 527
破壊応力 26 MPa ISO 527
破壊ひずみ 260 % ISO 527
曲げ弾性率, 23°C 2400 MPa ISO 178
曲げ強さ 83 MPa ISO 178
ノッチ付きIzod衝撃強さ, +23°C 7 kJ/m² ISO 180/1A
ロックウェル硬度 R 115 - ISO 2039-2
ASTM数据
降伏応力 60 MPa ASTM D 638
破壊応力 50 MPa ASTM D 638
降伏点伸び 5.3 % ASTM D 638
破断伸び 250 % ASTM D 638
曲げ弾性率 2403 MPa ASTM D 790
曲げ強さ 87.3 MPa ASTM D 790
ロックウェル硬度 R 115 - ASTM D 785
ノッチ付きIzod衝撃強さ, 1/8 in 60 J/m ASTM D 256
熱的特性単位テスト基準
ISO データ
荷重たわみ温度, 1.80 MPa 77 °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 89 °C ISO 75-1/-2
ASTM数据
DTUL @ 66 psi 79 °C ASTM D 648
DTUL @ 264 psi 68 °C ASTM D 648
光学特性単位テスト基準
ASTM数据
ヘイズ 1 % ASTM D 1003
視感透過率 86 % ASTM D 1003
その他の特性.単位テスト基準
密度. 1330 kg/m³ ISO 1183
密度 1330 kg/m³ ASTM D 792
特殊な特性
成形加工法.
フィルム押出成形., シート押出成形., ブロー成形.
特殊な特性.
熱安定化., 透明.
な特性
Amorphous, Copolymer
耐薬品性
General Chemical Resistance
Certifications
Contains renewable resources, RoHS
アプリケーション
パッケージング
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.