Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of ENGAGE™ 8411 - TPO - The Dow Chemical Company

Material Data Center offers the following functions for ENGAGE™ 8411:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Engage datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics単位テスト基準
ASTM数据
メルトフローレイト, MFI 18 g/10min ASTM D 1238
温度 190 °C -
荷重 2.16 kg -
機械的特性単位テスト基準
ASTM数据
破壊応力 7.3 MPa ASTM D 638
破断伸び 1000 % ASTM D 638
ショア硬さA 81 - ASTM D 2240
ショア硬さD 27 - ASTM D 2240
引裂強さ 47.5 kN/m ASTM D 624
熱的特性単位テスト基準
ASTM数据
溶融温度 76 °C ASTM D 3418
ガラス転移温度 -50 °C ASTM E 1356
ビカット軟化温度 45 °C ASTM D 1525
その他の特性.単位テスト基準
密度 880 kg/m³ ASTM D 792
特殊な特性
成形加工法.
射出成形., Compression Molding
納入形状.
ペレット.
特殊な特性.
透明.
な特性
Blending Resin, Low Odor
Certifications
Food contact, Food approval 10/2011, Food contact notification (FCN), US Pharmacopeia Class VI Approved, Drug Master File
アプリケーション
自動車
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ., 近東/アフリカ
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.