Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Hostacom EYC 772N - PP-MX - LyondellBasell Industries

Material Data Center offers the following functions for Hostacom EYC 772N:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Hostacom datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトフローレート, MFI 35 g/10min ISO 1133
温度 230 °C -
荷重 2.16 kg -
ASTM数据
メルトフローレイト, MFI 35 g/10min ASTM D 1238
温度 230 °C -
荷重 2.16 kg -
機械的特性単位テスト基準
ISO データ
降伏応力 25 MPa ISO 527
降伏ひずみ 4 % ISO 527
曲げ弾性率, 23°C 2300 MPa ISO 178
ノッチ付きIzod衝撃強さ, +23°C 7 kJ/m² ISO 180/1A
ASTM数据
降伏応力 25 MPa ASTM D 638
降伏点伸び 4.5 % ASTM D 638
破断伸び 18 % ASTM D 638
曲げ弾性率 2500 MPa ASTM D 790
Gardner衝撃 12.5 J ASTM D 2794,4226,5420
熱的特性単位テスト基準
ISO データ
荷重たわみ温度, 0.45 MPa 112 °C ISO 75-1/-2
ASTM数据
DTUL @ 66 psi 108 °C ASTM D 648
その他の特性.単位テスト基準
密度. 1040 kg/m³ ISO 1183
密度 1040 kg/m³ ASTM D 792
特殊な特性
成形加工法.
射出成形.
特殊な特性.
紫外線安定化.
な特性
Scratch Resistant, Copolymer
アプリケーション
自動車
領域別の利用可能性
北アメリカ.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.