Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Inzea® M28 - (PLA+PSAC) - Nurel S.A.

Material Data Center offers the following functions for Inzea® M28:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Inzea datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
more information can be found in the following table
Rilsamid® Chemical Resistance
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトボリュームレイト, MVR 10 cm³/10min ISO 1133
温度 190 °C -
荷重 2.16 kg -
光学特性単位テスト基準
ASTM数据
ヘイズ 80 % ASTM D 1003
その他の特性.単位テスト基準
Moisture Content 1 % -
機械的特性(ィルム)単位テスト基準
ISO データ
引張弾性率, 平行 120 MPa ISO 527-3
降伏応力, 平行 9 MPa ISO 527-3
降伏ひずみ, 平行 13 % ISO 527-3
破壊応力, 平行 27 MPa ISO 527-3
最大ひずみ, 平行 480 % ISO 527-3
トラウザー引裂抵抗, 直角 145 N/mm ISO 6383-1
押出成形のタイプ. blown - -
試験片の厚さ. 0.02 mm -
特殊な特性
成形加工法.
Blown Film Extrusion, フィルム押出成形., 熱成形.
Certifications
Contains renewable resources, Biodegradable, 堆肥化可能 ISO 13432 (プロデューサー), 堆肥化可能 ISO 13432 (証明書)
領域別の利用可能性
ヨーロッパ., 南・中央アメリカ.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.