Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of ISPLEN® PM284 AV - PP-MX20 - Repsol YPF S.A.

Material Data Center offers the following functions for ISPLEN® PM284 AV:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Isplen datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトフローレート, MFI 20 g/10min ISO 1133
温度 230 °C -
荷重 2.16 kg -
成形収縮率, 平行 0.7 % ISO 294-4, 2577
機械的特性単位テスト基準
ISO データ
引張弾性率 2000 MPa ISO 527
降伏応力 24 MPa ISO 527
降伏ひずみ 4 % ISO 527
破壊応力 19.5 MPa ISO 527
破壊ひずみ 25 % ISO 527
曲げ弾性率, 23°C 2350 MPa ISO 178
シャルピー衝撃強さ, +23°C 50 kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C 3 kJ/m² ISO 179/1eA
アイゾット衝撃試験, +23°C 40 kJ/m² ISO 180/1U
ノッチ付きIzod衝撃強さ, +23°C 4 kJ/m² ISO 180/1A
ショア硬さD 65 - ISO 7619-1
熱的特性単位テスト基準
ISO データ
荷重たわみ温度, 1.80 MPa 59 °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 95 °C ISO 75-1/-2
ビカット軟化温度, A 148 °C ISO 306
ビカット軟化温度, B 76 °C ISO 306
その他の特性.単位テスト基準
密度. 1040 kg/m³ ISO 1183
特殊な特性
特殊な特性.
高耐衝撃及び耐衝撃改良., 紫外線安定化.
な特性
Copolymer
アプリケーション
自動車
領域別の利用可能性
北アメリカ., ヨーロッパ., 南・中央アメリカ., 近東/アフリカ
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.