Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of KOPLA® KDG1015F - PA66-GF15 - KOPLA CO., LTD

Material Data Center offers the following functions for KOPLA® KDG1015F:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Kopla datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics単位テスト基準
ASTM数据
成形収縮率., 平行 0.0055 mm/mm ASTM D 955
成形収縮率, 直角 0.0085 mm/mm ASTM D 955
機械的特性乾燥/調湿単位テスト基準
ISO データ
シャルピー衝撃強さ, +23°C 45 / 52 kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C 8 / 9 kJ/m² ISO 179/1eA
ASTM数据
引張弾性率 5900 / 4600 MPa ASTM D 638
引張強度 115 / 85 MPa ASTM D 638
曲げ弾性率 5500 / 4100 MPa ASTM D 790
曲げ強さ 160 / 100 MPa ASTM D 790
ロックウェル硬度 R 120 / R 115 - ASTM D 785
熱的特性単位テスト基準
ASTM数据
UL94 燃焼性 V-0 - UL 94
線膨張係数, 平行 35 E-6/K ASTM D 696
DTUL @ 66 psi 238 °C ASTM D 648
DTUL @ 264 psi 220 °C ASTM D 648
溶融温度 260 °C ASTM D 3418
電気的特性.乾燥/調湿単位テスト基準
ASTM数据
耐電圧, 短い時間 40 / - kV/mm ASTM D 149
誘電正接, 1 MHz 0.02 / - - ASTM D 150
比誘電率, 1 MHz 3 / - - ASTM D 150
体積抵抗率 1E15 / - Ohm*cm ASTM D 257
その他の特性.単位テスト基準
吸水率, 24hr 0.8 % ASTM D 570
密度 1450 kg/m³ ASTM D 792
特殊な特性
特殊な特性.
難燃., 熱安定化.
アプリケーション
自動車, 電気電子
領域別の利用可能性
北アメリカ., アジア/太平洋地域.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.