Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Kynar Flex® Ultraflex B - PVDF - ARKEMA

Material Data Center offers the following functions for Kynar Flex® Ultraflex B:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Kynar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
Kynar Flex® resins are fluorinated thermoplastic copolymers.

Kynar Ultraflex® resin is a semi-crystalline copolymer of vinylidene fluoride and hexafluoropropylene. This copolymer is a highly flexible material that can be melt processed using typical melt processing equipment or can be easily put in solution for solution coating process. It can be supplied in as pellets for melt processing or as crumb to facilitate dissolution.

This is the most flexible Kynar Flex® resin grade available.

Additional characteristics:
- High flexibility
- Toughness
- Weatherability
- Solution properties
機械的特性単位テスト基準
ISO データ
引張弾性率 80 MPa ISO 527
降伏応力 6.5 MPa ISO 527
降伏ひずみ 20 % ISO 527
破壊呼びひずみ >50 % ISO 527
熱的特性単位テスト基準
ISO データ
溶融温度, 10°C/min 101 °C ISO 11357-1/-3
荷重たわみ温度, 1.80 MPa 46 °C ISO 75-1/-2
酸素指数 40 % ISO 4589-1/-2
その他の特性.単位テスト基準
吸水率 0.03 % Sim. to ISO 62
密度 1770 kg/m³ ISO 1183
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.