Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LOXIAMID PA6 LU HS1 03057 - PA6 - Loxim Industries Limited

Material Data Center offers the following functions for LOXIAMID PA6 LU HS1 03057:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Loxiamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトフローレート, MFI 17 g/10min ISO 1133
温度 225 °C -
荷重 2.16 kg -
機械的特性単位テスト基準
ISO データ
降伏応力 65 MPa ISO 527
破壊ひずみ 20 % ISO 527
曲げ弾性率, 23°C 2800 MPa ISO 178
曲げ強さ 95 MPa ISO 178
ノッチ付きIzod衝撃強さ, +23°C 7 kJ/m² ISO 180/1A
熱的特性単位テスト基準
ISO データ
荷重たわみ温度, 1.80 MPa 65 °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 130 °C ISO 75-1/-2
その他の特性.単位テスト基準
密度. 1130 kg/m³ ISO 1183
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 80 °C -
Pre-drying - Time 2 - 4 h -
Processing humidity ≤0.15 % -
樹脂温度 240 - 285 °C -
金型温度 65 - 80 °C -
特殊な特性
成形加工法.
射出成形.
添加剤.
滑剤., 離型剤.
特殊な特性.
高耐衝撃及び耐衝撃改良., 熱安定化.
耐薬品性
General Chemical Resistance
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.