Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Lucalen A 2700M - (PE-LD) - LyondellBasell Industries

Material Data Center offers the following functions for Lucalen A 2700M:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Lucalen datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトフローレート, MFI 7.2 g/10min ISO 1133
温度 190 °C -
荷重 2.16 kg -
機械的特性単位テスト基準
ISO データ
破壊応力 11 MPa ISO 527
破壊ひずみ >50 % ISO 527
曲げ弾性率, 23°C 42 MPa ISO 178
ノッチ付きIzod衝撃強さ N kJ/m² ISO 180/1A
温度 -40 °C -
ショア硬さD 30 - ISO 7619-1
熱的特性単位テスト基準
ISO データ
溶融温度, 10゚C/min 95 °C ISO 11357-1/-3
ビカット軟化温度, A 60 °C ISO 306
その他の特性.単位テスト基準
密度. 924 kg/m³ ISO 1183
特殊な特性
成形加工法.
射出成形., Blown Film Extrusion, フィルム押出成形., Pipe/Tube Extrusion, シート押出成形., Wire/Cable Extrusion, その他の押出成形., Compression Molding
納入形状.
ペレット., ナチュラルカラー
特殊な特性.
高耐衝撃及び耐衝撃改良.
な特性
Good Adhesion, Soft Feel, Weldable
耐薬品性
General Chemical Resistance, Environmental Stress Crack Resistance
Certifications
Food contact, Food approval 1935/2004/EC, Food approval 10/2011
領域別の利用可能性
ヨーロッパ., アジア/太平洋地域.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.