Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LUCEL HI515W - (POM+TPE) - LG Chem

Material Data Center offers the following functions for LUCEL HI515W:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Lucel datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics単位テスト基準
ASTM数据
メルトフローレイト, MFI 9 g/10min ASTM D 1238
温度 190 °C -
荷重 2.16 kg -
成形収縮率., 平行 0.0185 mm/mm ASTM D 955
機械的特性単位テスト基準
ASTM数据
降伏応力 41.9 MPa ASTM D 638
破断伸び 67 % ASTM D 638
曲げ弾性率 1419 MPa ASTM D 790
曲げ強さ 47.3 MPa ASTM D 790
ロックウェル硬度 R 64 - ASTM D 785
ノッチ付きIzod衝撃強さ, 1/4 in 69.7 J/m ASTM D 256
熱的特性単位テスト基準
ASTM数据
DTUL @ 264 psi 79 °C ASTM D 648
その他の特性.単位テスト基準
密度 1330 kg/m³ ASTM D 792
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 80 - 110 °C -
Pre-drying - Time 2 - 3 h -
Processing humidity ≤0.1 % -
樹脂温度 200 - 220 °C -
金型温度 80 - 110 °C -
Zone 1 160 - 180 °C -
Zone 2 170 - 190 °C -
Zone 3 180 - 200 °C -
Nozzle temperature 180 - 200 °C -
Screw speed 80 - 110 rpm -
Back pressure 0.5 - 3 MPa -
特殊な特性
成形加工法.
射出成形.
特殊な特性.
高耐衝撃及び耐衝撃改良.
アプリケーション
自動車
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com