Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LUCON PO-6062 - PPO-(CF+GF)... - LG Chem

Material Data Center offers the following functions for LUCON PO-6062:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Lucon datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics単位テスト基準
ASTM数据
メルトフローレイト, MFI 2 g/10min ASTM D 1238
温度 300 °C -
荷重 2.16 kg -
成形収縮率., 平行 0.002 mm/mm ASTM D 955
機械的特性単位テスト基準
ASTM数据
降伏応力 167 MPa ASTM D 638
破断伸び 8 % ASTM D 638
曲げ弾性率 9810 MPa ASTM D 790
曲げ強さ 235 MPa ASTM D 790
ノッチ付きIzod衝撃強さ, 1/8 in 88.3 J/m ASTM D 256
熱的特性単位テスト基準
ASTM数据
DTUL @ 264 psi 195 °C ASTM D 648
電気的特性.単位テスト基準
ASTM数据
表面抵抗率 1000000 Ohm ASTM D 257
その他の特性.単位テスト基準
密度 1300 kg/m³ ASTM D 792
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 90 - 110 °C -
Pre-drying - Time 4 - 5 h -
樹脂温度 280 - 300 °C -
金型温度 90 - 120 °C -
Zone 1 270 - 290 °C -
Zone 2 280 - 300 °C -
Zone 3 280 - 310 °C -
Nozzle temperature 280 - 300 °C -
Screw speed 40 - 60 rpm -
Back pressure 0 - 1 MPa -
特殊な特性
成形加工法.
射出成形.
特殊な特性.
熱安定化.
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.