Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Luran® S 797SE Q440 - ASA - INEOS Styrolution

Material Data Center offers the following functions for Luran® S 797SE Q440:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, cooling time calculation, CAE Interfaces

Check here, which other Luran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
Luran® S 797SE Q440 acrylonitrile styrene acrylate (ASA) polymer features high surface quality and good impact strength including enhanced colour fastness. The product delivers superior long-term performance when exposed to UV irradiation and additionally provide excellent chemical resistance. Luran® S 797SE Q440 is an extrusion grade providing high impact strength and enhanced UV resistance. It is suitable for co-extrusion with ABS or PVC enabling a low gloss surface finish.
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトボリュームレイト, MVR 5 cm³/10min ISO 1133
温度 220 °C -
荷重 10 kg -
溶融時の密度 967 kg/m³ -
溶融時の熱伝導率 0.204 W/(m K) -
溶融時の比熱 2830 J/(kg K) -
機械的特性単位テスト基準
ISO データ
引張弾性率 1900 MPa ISO 527
降伏応力 41 MPa ISO 527
降伏ひずみ 3.5 % ISO 527
破壊呼びひずみ 8.6 % ISO 527
シャルピー衝撃強さ, +23°C 210 kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C 20 kJ/m² ISO 179/1eA
ノッチ付きシャルピー衝撃強さ, -30°C 5 kJ/m² ISO 179/1eA
熱的特性単位テスト基準
ISO データ
荷重たわみ温度, 1.80 MPa 96 °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 101 °C ISO 75-1/-2
ビカット軟化温度, A 102 °C ISO 306
ビカット軟化温度, B 92 °C ISO 306
線膨張係数, 平行 95 E-6/K ISO 11359-1/-2
電気的特性.単位テスト基準
ISO データ
比誘電率, 100Hz 3.8 - IEC 62631-2-1
誘電正接, 100Hz 90 E-4 IEC 62631-2-1
その他の特性.単位テスト基準
吸湿率 0.4 % Sim. to ISO 62
密度 1070 kg/m³ ISO 1183
Bulk density 600 kg/m³ -
Processing Recommendation Extrusion単位テスト基準
Type of extrusion profile - -
Pre-drying - Temperature 80 °C -
Pre-drying - Time 2 - 4 h -
樹脂温度 200 - 240 °C -
Type of extrusion sheet - -
Pre-drying - Temperature 80 °C -
Pre-drying - Time 2 - 4 h -
樹脂温度 210 - 250 °C -
特殊な特性
成形加工法.
異形押出成形., シート押出成形., その他の押出成形.
納入形状.
ペレット.
特殊な特性.
高耐衝撃及び耐衝撃改良., 光安定化., 紫外線安定化., 熱安定化.
耐薬品性
General Chemical Resistance
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ., 近東/アフリカ
その他の情報
村遜速揃
その他の押出成形.
PREPROCESSING

Pre-drying, Temperature: 80°C

Pre-drying, Time: 2 - 4h

PROCESSING

Extrusion, Pipes, Melt temperature: 200 - 240°C

族臓遜造揃
PREPROCESSING

Pre-drying, Temperature: 80°C

Pre-drying, Time: 2 - 4h

PROCESSING

Extrusion, Profiles, Melt temperature: 200 - 240°C

促揃臓村促速揃
PREPROCESSING

Pre-drying, Temperature: 80°C

Pre-drying, Time: 2 - 4h

PROCESSING

Extrusion, Plates, Melt temperature: 210 - 250°C

Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.