Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Luran® S ECO 776SE BC40 - ASA - INEOS Styrolution

Material Data Center offers the following functions for Luran® S ECO 776SE BC40:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Luran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
Luran® S ECO 776SE BC40 acrylonitrile styrene acrylate (ASA) polymer features high surface quality and good impact strength including enhanced colour fastness. The product delivers superior long-term performance when exposed to UV irradiation and additionally provide excellent chemical resistance. Luran® S ECO 776SE BC40 is suitable extrusion applications. It provides good impact toughness and enables matte surface appearance for extruded sheets. Luran® S ECO 776SE BC40 is an ISCC compliant product leading to a substitution of fossil source styrene with ISCC certified bio-attributed styrene.
Carbon Footprint Reduction vs Fossil-Based (3rd party validated): 53 % (ISO 14044)
Attributed Content of ISCC-certified Bio-Circular Sources (min.): 40 %
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトボリュームレイト, MVR 4 cm³/10min ISO 1133
温度 220 °C -
荷重 10 kg -
溶融時の熱伝導率 0.17 W/(m K) -
機械的特性単位テスト基準
ISO データ
引張弾性率 2200 MPa ISO 527
降伏応力 47 MPa ISO 527
降伏ひずみ 3.3 % ISO 527
破壊呼びひずみ 12 % ISO 527
曲げ弾性率, 23°C 2000 MPa ISO 178
曲げ強さ 65 MPa ISO 178
シャルピー衝撃強さ, +23°C N kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C 30 kJ/m² ISO 179/1eA
ノッチ付きシャルピー衝撃強さ, -30°C 4 kJ/m² ISO 179/1eA
Ball indentation hardness 70 MPa ISO 2039-1
熱的特性単位テスト基準
ISO データ
荷重たわみ温度, 1.80 MPa 96 °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 101 °C ISO 75-1/-2
ビカット軟化温度, B 92 °C ISO 306
線膨張係数, 平行 95 E-6/K ISO 11359-1/-2
1.5mm厚さでの燃焼性 HB class IEC 60695-11-10
試験片の厚さ 1.5 mm -
Yellow Card 可用 はい - -
厚さhでの燃焼性 HB class IEC 60695-11-10
試験片の厚さ 3.0 mm -
燃焼速度, FMVSS, 1mm厚 25[1] mm/min ISO 3795 (FMVSS 302)
酸素指数 19 % ISO 4589-1/-2
Other Standards[S]
熱伝導率, ソリッド 0.17 W/(m K) DIN 52612-1
1: 2 mm  S: These properties are reported by the producer according standards that are different to our defaults.
その他の特性.単位テスト基準
吸水率 1.65 % Sim. to ISO 62
吸湿率 0.35 % Sim. to ISO 62
密度 1070 kg/m³ ISO 1183
Bulk density 600 kg/m³ -
Processing Recommendation Extrusion単位テスト基準
Type of extrusion profile - -
Pre-drying - Temperature 80 °C -
Pre-drying - Time 2 - 4 h -
樹脂温度 240 °C -
Type of extrusion sheet - -
Pre-drying - Temperature 80 °C -
Pre-drying - Time 2 - 4 h -
樹脂温度 210 - 250 °C -
機能
 応力-ひずみ. , Luran® S ECO 776SE BC40, ASA, INEOS Styrolution
 割線弾性率−ひずみ. , Luran® S ECO 776SE BC40, ASA, INEOS Styrolution
 応力-ひずみ (等時的). 23°C, Luran® S ECO 776SE BC40, ASA, INEOS Styrolution
 クリープ弾性率−時間. 23°C, Luran® S ECO 776SE BC40, ASA, INEOS Styrolution
クリープ曲線 23°C, Luran® S ECO 776SE BC40, ASA, INEOS Styrolution
 応力-ひずみ (等時的). 40°C, Luran® S ECO 776SE BC40, ASA, INEOS Styrolution
 クリープ弾性率−時間. 40°C, Luran® S ECO 776SE BC40, ASA, INEOS Styrolution
クリープ曲線 40°C, Luran® S ECO 776SE BC40, ASA, INEOS Styrolution
 応力-ひずみ (等時的). 60°C, Luran® S ECO 776SE BC40, ASA, INEOS Styrolution
 クリープ弾性率−時間. 60°C, Luran® S ECO 776SE BC40, ASA, INEOS Styrolution
クリープ曲線 60°C, Luran® S ECO 776SE BC40, ASA, INEOS Styrolution
 応力-ひずみ (等時的). 80°C, Luran® S ECO 776SE BC40, ASA, INEOS Styrolution
 クリープ弾性率−時間. 80°C, Luran® S ECO 776SE BC40, ASA, INEOS Styrolution
クリープ曲線 80°C, Luran® S ECO 776SE BC40, ASA, INEOS Styrolution
 pvT , Luran® S ECO 776SE BC40, ASA, INEOS Styrolution
 引張弾性率-温度. , Luran® S ECO 776SE BC40, ASA, INEOS Styrolution
特殊な特性
成形加工法.
異形押出成形., シート押出成形., その他の押出成形., ブロー成形., 熱成形.
納入形状.
ペレット.
特殊な特性.
高耐衝撃及び耐衝撃改良., 光安定化., 紫外線安定化., 熱安定化.
耐薬品性
General Chemical Resistance
Certifications
Contains renewable resources, ISCC Plus
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ., 近東/アフリカ
その他の情報
村遜速揃
その他の押出成形.
PREPROCESSING

Pre-drying, Temperature: 80°C

Pre-drying, Time: 2 - 4h

PROCESSING

Extrusion, Pipes, Melt temperature: 200 - 240°C

族臓遜造揃
PREPROCESSING

Pre-drying, Temperature: 80°C

Pre-drying, Time: 2 - 4h

PROCESSING

Extrusion, Profiles, Melt temperature: 240°C

促揃臓村促速揃
PREPROCESSING

Pre-drying, Temperature: 80°C

Pre-drying, Time: 2 - 4h

PROCESSING

Extrusion, Plates, Melt temperature: 210 - 250°C

Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com