Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LUTENE XL2808BK - PE - LG Chem

Material Data Center offers the following functions for LUTENE XL2808BK:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Lutene datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
LUTENE® XL2808BK has an excellent electrical properties and assists in obtaining a minimum shrink back on aluminum conductor, especially solid conductor. LUTENE® XL2808BK is specifically developed to provide a smooth surface yielding a more perfect interface between the extruded shield and the insulation.

LUTENE® XL2808BK has stable volume resistivity characteristics at elevated temperatures and is formulated with a polymer system that has demonstrated compatibility with copper conductor.

機械的特性単位テスト基準
ASTM数据
引張強度 16.7 MPa ASTM D 638
破断伸び 200 % ASTM D 638
電気的特性.単位テスト基準
Other Standards[S]
体積抵抗率 100 Ohm*cm ASTM D991
S: These properties are reported by the producer according standards that are different to our defaults.
その他の特性.単位テスト基準
密度 1140 kg/m³ ASTM D 792
Moisture Content 0.05 % -
Processing Recommendation Extrusion単位テスト基準
Pre-drying - Temperature 60 - 70 °C -
Pre-drying - Time 4 h -
樹脂温度 100 - 125 °C -
特殊な特性
成形加工法.
その他の押出成形.
納入形状.
な特性
Crosslinkable, EMI Attenuation/Shielding
アプリケーション
電気電子
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.