Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of MAGNUM™ 1250 BG - ABS - Trinseo

Material Data Center offers the following functions for MAGNUM™ 1250 BG:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Magnum datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトフローレート, MFI 1.7 g/10min ISO 1133
温度 220 °C -
荷重 10 kg -
ASTM数据
メルトフローレイト, MFI 1.7 g/10min ASTM D 1238
温度 230 °C -
荷重 3.8 kg -
機械的特性単位テスト基準
ISO データ
降伏応力 33.7 MPa ISO 527
曲げ弾性率, 23°C 1810 MPa ISO 178
ノッチ付きIzod衝撃強さ, +23°C 26 kJ/m² ISO 180/1A
ノッチ付きIzod衝撃強さ 17 kJ/m² ISO 180/1A
温度 -30 °C -
ASTM数据
降伏応力 33.6 MPa ASTM D 638
破断伸び 60 % ASTM D 638
曲げ弾性率 2013 MPa ASTM D 790
ノッチ付きIzod衝撃強さ, 1/8 in 358 J/m ASTM D 256
ノッチ付きIzod衝撃強さ, Low-Temperature 187 J/m ASTM D 256
温度 -28.9 °C -
熱的特性単位テスト基準
ISO データ
荷重たわみ温度, 1.80 MPa 85 °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 101 °C ISO 75-1/-2
ASTM数据
DTUL @ 66 psi 103 °C ASTM D 648
DTUL @ 264 psi 86.7 °C ASTM D 648
その他の特性.単位テスト基準
密度 1050 kg/m³ ASTM D 792
特殊な特性
成形加工法.
ブロー成形.
特殊な特性.
高耐衝撃及び耐衝撃改良., 熱安定化.
領域別の利用可能性
北アメリカ.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.