Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NORYL™ Resin EN185 - Americas - (PPE+PS) - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for NORYL™ Resin EN185 - Americas:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Noryl datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
NORYL™ EN185 resin is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This extrusion grade contains non-brominated, non-chlorinated flame retardant and carries a UL94 flame rating of v0 at 3mm and V1 at 1.5mm. NORYL EN185 resin exhibits excellent impact strength, very low moisture absorption, good dimensional stability, and great machinability. NORYL EN185 resin is an excellent candidate for a variety of applications including fiber optic ducting,

UL Yellow Card Link E121562-221153
機械的特性単位テスト基準
ASTM数据
降伏応力 42 MPa ASTM D 638
破断伸び 50 % ASTM D 638
ロックウェル硬度 R 113 - ASTM D 785
ノッチ付きIzod衝撃強さ, 1/8 in 389 J/m ASTM D 256
ノッチ付きIzod衝撃強さ, Low-Temperature 160 J/m ASTM D 256
温度 -40 °C -
熱的特性単位テスト基準
ISO データ
1.5mm厚さでの燃焼性 V-1 class IEC 60695-11-10
試験片の厚さ 1.5 mm -
厚さhでの燃焼性 V-0 class IEC 60695-11-10
試験片の厚さ 3.0 mm -
電気的特性.単位テスト基準
ISO データ
誘電正接, 1MHz 35 E-4 IEC 62631-2-1
ASTM数据
耐電圧, 短い時間 24.8 kV/mm ASTM D 149
誘電正接, 60 Hz 0.004 - ASTM D 150
比誘電率, 60 Hz 2.8 - ASTM D 150
その他の特性.単位テスト基準
密度 1080 kg/m³ ASTM D 792
特殊な特性
添加剤.
難燃剤.
特殊な特性.
難燃.
領域別の利用可能性
北アメリカ.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.