Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Pebax® 3533 SA 01 MED - TPA - ARKEMA

Material Data Center offers the following functions for Pebax® 3533 SA 01 MED:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Pebax datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
Polyether block amide Pebax® 3533 SA 01 MED resin is a thermoplastic elastomer made of flexible polyether and rigid polyamide.
This grade offers the highest quality and it is specially designed to meet the stringent requirements of the medical applications such as minimally invasive devices.
Upon request, letters regarding USP Class VI compliance can be provided.


Main applications:
  • Catheters
  • Flexible injected parts


Packaging:

This grade is delivered dried in sealed packaging (25 kg bags) ready to be processed.

Shelf Life:
Two years from the delivery. For any use above this limit, please refer to our technical services.
機械的特性乾燥/調湿単位テスト基準
ISO データ
引張弾性率 19 / 18 MPa ISO 527
50%ひずみ時応力 4 / 4 MPa ISO 527
破壊ひずみ >50 / >50 % ISO 527
破壊応力 TPE 39 / * MPa ISO 527
破壊ひずみ TPE >300 / * % ISO 527
ショア硬さA 80 / * - ISO 7619-1
ショア硬さD 25 / * - ISO 7619-1
熱的特性乾燥/調湿単位テスト基準
ISO データ
溶融温度, 10°C/min 144 / * °C ISO 11357-1/-3
その他の特性.乾燥/調湿単位テスト基準
吸水率 1.2 / * % Sim. to ISO 62
吸湿率 0.4 / * % Sim. to ISO 62
密度 1000 / 1000 kg/m³ ISO 1183
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 55 - 65 °C -
Pre-drying - Time 4 - 8 h -
樹脂温度 180 - 240 °C -
金型温度 10 - 30 °C -
特殊な特性
成形加工法.
射出成形., フィルム押出成形., その他の押出成形.
納入形状.
ペレット.
添加剤.
滑剤.
特殊な特性.
熱安定化.
Certifications
Medical Grade, US Pharmacopeia Class VI Approved
領域別の利用可能性
その他の情報
村遜速揃

Processing conditions:

- Typical melt temperature (Min / Recommended / Max) : 180°C / 210°C / 240°C.
- Typical mold temperature : 10 – 30°C.
- Drying time and temperature (only necessary for bags opened for more than two hours) : 4-8 hours at 55-65°C.
その他の押出成形.

Processing conditions:

- Typical melt temperature (Min / Recommended / Max) : 190°C / 205°C / 220°C.
- Drying time and temperature (only necessary for bags opened for more than two hours) : 4-8 hours at 55-65°C.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.