Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Pebax® 6333 SA 01 MED - TPA - ARKEMA

Material Data Center offers the following functions for Pebax® 6333 SA 01 MED:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Pebax datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
Polyether block amide Pebax® 6333 SA 01 MED resin is a thermoplastic elastomer made of flexible polyether and rigid polyamide.
This grade offers the highest quality and it is specially designed to meet the stringent requirements of the medical applications such as minimally invasive devices.
Pebax® 6333 SA 01 MED resin also offers an excellent combination of properties such as: kink resistance, low friction coefficient and superior dynamic response.
Upon request, letters regarding USP Class VI compliance can be provided.


Main applications:
  • Tubings like angiography and angioplasty catheters
  • Flexible injected parts


Packaging:

This grade is delivered dried in sealed packaging (20 kg bags) ready to be processed.

Shelf Life:
Two years from the delivery. For any use above this limit, please refer to our technical services.
機械的特性乾燥/調湿単位テスト基準
ISO データ
引張弾性率 307 / 240 MPa ISO 527
降伏応力 19 / 18 MPa ISO 527
降伏ひずみ 22 / 22 % ISO 527
破壊呼びひずみ >50 / >50 % ISO 527
ノッチ付きシャルピー衝撃強さ, -30°C - / 20 kJ/m² ISO 179/1eA
ショア硬さD 58 / * - ISO 7619-1
熱的特性乾燥/調湿単位テスト基準
ISO データ
溶融温度, 10°C/min 169 / * °C ISO 11357-1/-3
ビカット軟化温度, B 85 / * °C ISO 306
その他の特性.乾燥/調湿単位テスト基準
吸水率 1.1 / * % Sim. to ISO 62
吸湿率 0.7 / * % Sim. to ISO 62
密度 1010 / - kg/m³ ISO 1183
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 65 - 75 °C -
Pre-drying - Time 4 - 6 h -
樹脂温度 230 - 290 °C -
金型温度 25 - 60 °C -
特殊な特性
成形加工法.
射出成形., その他の押出成形.
納入形状.
ペレット.
特殊な特性.
光安定化., 熱安定化.
Certifications
Medical Grade, US Pharmacopeia Class VI Approved
領域別の利用可能性
その他の情報
村遜速揃

Processing conditions:

- Typical melt temperature (Min / Recommended / Max) : 230°C / 260°C / 290°C.
- Typical mold temperature : 25 – 60°C.
- Drying time and temperature (only necessary for bags opened for more than two hours) : 4-6 hours at 65-75°C.
その他の押出成形.

Processing conditions:

- Typical melt temperature (Min / Recommended / Max) : 210°C / 225°C / 240°C.
- Drying time and temperature (only necessary for bags opened for more than two hours) : 4-6 hours at 65-75°C.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.