Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Plenco 02571 - PF-X - Plastics Engineering Co.

Material Data Center offers the following functions for Plenco 02571:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Plenco datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics単位テスト基準
ASTM数据
成形収縮率., 平行 0.0089 mm/mm ASTM D 955
機械的特性単位テスト基準
ASTM数据
引張弾性率 8741 MPa ASTM D 638
引張強度 61 MPa ASTM D 638
圧縮強度 191 MPa ASTM D 695
曲げ弾性率 7654 MPa ASTM D 790
曲げ強さ 90.5 MPa ASTM D 790
ロックウェル硬度 E 86 - ASTM D 785
ノッチ付きIzod衝撃強さ, 1/8 in 18.7 J/m ASTM D 256
熱的特性単位テスト基準
ASTM数据
UL94 燃焼性 HB - UL 94
追加試験片の厚さ 1.5 mm -
DTUL @ 264 psi 157 °C ASTM D 648
酸素指数 24.5 % ASTM D 2863
電気的特性.単位テスト基準
ASTM数据
耐電圧, 短い時間 12.9 kV/mm ASTM D 149
誘電正接, 1 MHz 0.046 - ASTM D 150
比誘電率, 1 MHz 4.6 - ASTM D 150
体積抵抗率 3E12 Ohm*cm ASTM D 257
耐アーク 136 s ASTM D 495
その他の特性.単位テスト基準
密度 1410 kg/m³ ASTM D 792
特殊な特性
成形加工法.
射出成形.
納入形状.
顆粒., 黒
アプリケーション
電気電子, 汎用
領域別の利用可能性
北アメリカ.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.