Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of RamOfin PPC341T4NT - PP-T20 - Polyram

Material Data Center offers the following functions for RamOfin PPC341T4NT:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Ramofin datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトフローレート, MFI 3.3 g/10min ISO 1133
温度 230 °C -
荷重 2.16 kg -
Other Standards[S]
成形収縮率, 平行 1.0 % Producer Method
S: These properties are reported by the producer according standards that are different to our defaults.
機械的特性単位テスト基準
ISO データ
引張弾性率 1850 MPa ISO 527
引張強度 24.5 MPa ISO 527
降伏ひずみ 4.9 % ISO 527
ノッチ付きIzod衝撃強さ, +23°C 5.7 kJ/m² ISO 180/1A
その他の特性.単位テスト基準
密度. 1040 kg/m³ ISO 1183
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 80 °C -
Pre-drying - Time 2 - 4 h -
Processing humidity ≤0.1 % -
金型温度 30 - 70 °C -
Feed temperature 60 - 70 °C -
Zone 1 200 - 230 °C -
Zone 2 200 - 230 °C -
Zone 3 200 - 250 °C -
特殊な特性
成形加工法.
射出成形.
納入形状.
ナチュラルカラー
な特性
Copolymer
Certifications
RoHS
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ., 近東/アフリカ
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.