Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Rilsamid® AESNO P401 TL - PA12 - ARKEMA

Material Data Center offers the following functions for Rilsamid® AESNO P401 TL:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Rilsamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
ISO 16396 - PA12-P, EGHL, C22-004

Rilsamid® AESNO P401 TL resin is a natural polyamide. 
This grade is plasticized and designed for tube extrusion.

Rilsamid® AESNO P401 TL resin falls into the PA12-HIPHL category according to DIN 73378.


Main applications:

Tubings

Packaging:
This grade is delivered dried in sealed packaging (44 lb bags / 1000 lb containers) ready to be processed.

Shelf life:
Two years from the date of delivery. for any use above this limit, please refer to our technical services.
Processing/Physical Characteristics乾燥/調湿単位テスト基準
ISO データ
メルトボリュームレイト, MVR 13 / * cm³/10min ISO 1133
温度 235 / * °C -
荷重 5 / * kg -
機械的特性乾燥/調湿単位テスト基準
ISO データ
引張弾性率 - / 360 MPa ISO 527
50%ひずみ時応力 - / 24 MPa ISO 527
破壊ひずみ - / >50 % ISO 527
ノッチ付きシャルピー衝撃強さ, +23°C 46 / - kJ/m² ISO 179/1eA
ノッチ付きシャルピー衝撃強さ, -30°C 4 / 8 kJ/m² ISO 179/1eA
熱的特性乾燥/調湿単位テスト基準
ISO データ
溶融温度, 10°C/min 174 / * °C ISO 11357-1/-3
電気的特性.乾燥/調湿単位テスト基準
ISO データ
耐電圧 41 / - kV/mm IEC 60243-1
耐トラッキング性 600 / - - IEC 60112
その他の特性.乾燥/調湿単位テスト基準
吸水率 1.2 / * % Sim. to ISO 62
密度 1030 / - kg/m³ ISO 1183
Processing Recommendation Extrusion単位テスト基準
Pre-drying - Temperature 80 °C -
Pre-drying - Time 4 - 6 h -
樹脂温度 230 - 270 °C -
特殊な特性
成形加工法.
Pipe/Tube Extrusion
添加剤.
可塑剤.
領域別の利用可能性
その他の情報
その他の押出成形.

Processing conditions for extrusion :

- Typical melt temperature (Min / Recommended / Max) : 230°C / 250°C / 270°C.
- Drying time and temperature (only necessary for bags opened for more than two hours) : 4-6 hours at 80°C.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.