Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Rilsamid® AZM 30 O TLD - PA12-GF30 - ARKEMA

Material Data Center offers the following functions for Rilsamid® AZM 30 O TLD:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Rilsamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
ISO 16396 - PA12 , GF30, M1GHLR, C16-070

Rilsamid® AZM 30 O TLD resin is a fiberglass reinforced polyamide. This natural grade is designed for injection moulding.

This grade is also available in green (Rilsamid® AZM 30 Green 56827 TLD resin) and grey (Rilsamid® AZM 30 Grey 632 TLD resin).




Packaging: 
This grade is delivered dried in sealed packaging (25 kg bags) ready to be processed

Shelf life: 
Two years from the delivery.
For any use above this limit please refer to our technical services. 
Processing/Physical Characteristics乾燥/調湿単位テスト基準
ISO データ
メルトボリュームレイト, MVR 12 / * cm³/10min ISO 1133
温度 235 / * °C -
荷重 5 / * kg -
機械的特性乾燥/調湿単位テスト基準
ISO データ
引張弾性率 6900 / 6500 MPa ISO 527
破壊応力 122 / 110 MPa ISO 527
破壊ひずみ 5 / 6 % ISO 527
シャルピー衝撃強さ, +23°C 85 / 88 kJ/m² ISO 179/1eU
シャルピー衝撃強さ, -30°C 96 / 93 kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C 23 / 22 kJ/m² ISO 179/1eA
ノッチ付きシャルピー衝撃強さ, -30°C 15 / 16 kJ/m² ISO 179/1eA
熱的特性乾燥/調湿単位テスト基準
ISO データ
溶融温度, 10°C/min 179 / * °C ISO 11357-1/-3
荷重たわみ温度, 1.80 MPa 160 / * °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 175 / * °C ISO 75-1/-2
ビカット軟化温度, B 165 / * °C ISO 306
線膨張係数, 平行 50 / * E-6/K ISO 11359-1/-2
電気的特性.乾燥/調湿単位テスト基準
ISO データ
比誘電率, 100Hz 4 / - - IEC 62631-2-1
比誘電率, 1MHz 4 / - - IEC 62631-2-1
誘電正接, 100Hz 752 / - E-4 IEC 62631-2-1
誘電正接, 1MHz 251 / - E-4 IEC 62631-2-1
体積抵抗率 - / 1E11 Ohm*m IEC 62631-3-1
表面抵抗率 * / 1E14 Ohm IEC 62631-3-2
耐電圧 - / 45 kV/mm IEC 60243-1
耐トラッキング性 * / 600 - IEC 60112
その他の特性.乾燥/調湿単位テスト基準
吸水率 1.2 / * % Sim. to ISO 62
吸湿率 0.6 / * % Sim. to ISO 62
密度 1230 / 1230 kg/m³ ISO 1183
機能
 粘度せん断速度. , Rilsamid® AZM 30 O TLD, PA12-GF30, ARKEMA
 せん断応力-せん断速度. , Rilsamid® AZM 30 O TLD, PA12-GF30, ARKEMA
 応力-ひずみ (等時的). 23°C, Rilsamid® AZM 30 O TLD (乾燥), PA12-GF30, ARKEMA
 クリープ弾性率−時間. 23°C, Rilsamid® AZM 30 O TLD (乾燥), PA12-GF30, ARKEMA
クリープ曲線 23°C, Rilsamid® AZM 30 O TLD (乾燥), PA12-GF30, ARKEMA
特殊な特性
成形加工法.
射出成形.
納入形状.
ペレット.
添加剤.
離型剤.
特殊な特性.
光安定化., 紫外線安定化., 熱安定化.
領域別の利用可能性
その他の情報
村遜速揃

Processing conditions:

- Typical melt temperature (Min / Recommended / Max) : 250°C / 265°C / 280°C.
- Typical mold temperature : 40 – 90°C.
- Drying time and temperature (only necessary for bags opened for more than two hours) : 4-8 hours at 80-90°C.

Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.