Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Rilsan® HT CSR13 - PA*-CF15 - ARKEMA

Material Data Center offers the following functions for Rilsan® HT CSR13:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Rilsan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
PA11/10T,CF13,MHL, C16-080

Rilsan® HT CSR 13 is a flexible polyphthalamide produced from a renewable source. This grade is fiber reinforced formulated for high-temperature applications requiring static charge dissipation and designed for injection molding.

According to ASTM D6866, the biobased carbon content is measured at 52%.



Main applications:
  • Conductive automotive & transportation quick connector

Packaging:
This grade is delivered dried in sealed packaging (25 kg bags) ready to be processed.

Shelf Life:
Two years from the delivery. For any use above this limit,  please refer to our technical services.
Processing/Physical Characteristics乾燥/調湿単位テスト基準
ISO データ
メルトボリュームレイト, MVR 12 / * cm³/10min ISO 1133
温度 275 / * °C -
荷重 2.16 / * kg -
成形収縮率, 平行 0.3 / * % ISO 294-4, 2577
成形収縮率, 直角 0.6 / * % ISO 294-4, 2577
機械的特性乾燥/調湿単位テスト基準
ISO データ
引張弾性率 - / 7600 MPa ISO 527
破壊応力 - / 151 MPa ISO 527
破壊ひずみ - / 2 % ISO 527
シャルピー衝撃強さ, +23°C - / 40 kJ/m² ISO 179/1eU
シャルピー衝撃強さ, -30°C - / 32 kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C - / 5 kJ/m² ISO 179/1eA
ノッチ付きシャルピー衝撃強さ, -30°C - / 4 kJ/m² ISO 179/1eA
熱的特性乾燥/調湿単位テスト基準
ISO データ
溶融温度, 10°C/min 255 / * °C ISO 11357-1/-3
荷重たわみ温度, 1.80 MPa 195 / * °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 235 / * °C ISO 75-1/-2
その他の特性.乾燥/調湿単位テスト基準
密度 1150 / 1150 kg/m³ ISO 1183
Biobased content 54 % -
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 100 - 110 °C -
Pre-drying - Time 4 - 8 h -
樹脂温度 270 - 320 °C -
金型温度 80 - 110 °C -
特殊な特性
成形加工法.
射出成形.
納入形状.
ペレット.
特殊な特性.
導電.
Certifications
Contains renewable resources
その他の情報
村遜速揃
Processing conditions :
- Typical melt temperature (Min / Recommanded / Maxi) : 270°C  / 280°C / 320°C.
- Typical mold temperature : 80 - 110°C.
- Drying time and temperature (only for bags opened for more than two hours) : 4 - 8 hours / 100 - 110°C.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.