Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SCANBLEND P AP2060 F30B - (PBT+ASA)-GF30 - Polykemi AB

Material Data Center offers the following functions for SCANBLEND P AP2060 F30B:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Scanblend datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトフローレート, MFI 12 g/10min ISO 1133
温度 275 °C -
荷重 2.16 kg -
成形収縮率, 平行 0.2 % ISO 294-4, 2577
成形収縮率, 直角 0.7 % ISO 294-4, 2577
機械的特性単位テスト基準
ISO データ
引張強度 114 MPa ISO 527
降伏ひずみ 7 % ISO 527
破壊ひずみ 8 % ISO 527
曲げ弾性率, 23°C 9800 MPa ISO 178
シャルピー衝撃強さ, +23°C 48 kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C 10 kJ/m² ISO 179/1eA
熱的特性単位テスト基準
ISO データ
荷重たわみ温度, 1.80 MPa 195 °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 215 °C ISO 75-1/-2
ビカット軟化温度, A 215 °C ISO 306
ビカット軟化温度, B 185 °C ISO 306
1.5mm厚さでの燃焼性 HB class IEC 60695-11-10
試験片の厚さ 1.6 mm -
グローワイヤ着火温度 (GWIT) 750 °C IEC 60695-2-13
GWIT - 試験片の厚さ 2 mm -
その他の特性.単位テスト基準
密度. 1480 kg/m³ ISO 1183
特殊な特性
成形加工法.
射出成形.
納入形状.
顆粒.
領域別の利用可能性
ヨーロッパ., アジア/太平洋地域.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com