Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SINKRAL® B4 Milano - ABS - Versalis S.p.A

Material Data Center offers the following functions for SINKRAL® B4 Milano:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Sinkral datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文

Symbol according to ISO 1043-1: ABS

Designation: Thermoplastics ISO 2580-ABS 1,EGN,105-04-16-20

Sinkral B 4 Milano is a special grade for extrusion/thermoforming.
Thanks to its low gel content toghether an optimum balance of stiffness and impact resistance, ensures high aesthetic quality of surfaces, partcularly suitable for co-extrusion.
Optimal thermal stability and rheological properties also permit the sheet production of large dimensions.


Applications:

Exstruded and co-exstruded sheets, including thick sheet where high hot draw ratios are required.
Its excellent surface appearance permit the use in a wide range of applications such as furniture, refrigerator, sanitary, automotive and packaging for foodstuff and industrial items.
Also ideal for the extrusion of profiles for furniture industry.

 

Processing/Physical Characteristics単位テスト基準
ISO データ
メルトボリュームレイト, MVR 4 cm³/10min ISO 1133
温度 220 °C -
荷重 10 kg -
溶融時の密度 960 kg/m³ -
溶融時の比熱 2150 J/(kg K) -
機械的特性単位テスト基準
ISO データ
引張弾性率 2300 MPa ISO 527
降伏応力 45 MPa ISO 527
降伏ひずみ 3 % ISO 527
破壊呼びひずみ 30 % ISO 527
シャルピー衝撃強さ, +23°C N kJ/m² ISO 179/1eU
シャルピー衝撃強さ, -30°C 140 kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C 18 kJ/m² ISO 179/1eA
ノッチ付きシャルピー衝撃強さ, -30°C 8 kJ/m² ISO 179/1eA
熱的特性単位テスト基準
ISO データ
ガラス転移点, 10°C/min 109 °C ISO 11357-1/-2
荷重たわみ温度, 1.80 MPa 83 °C ISO 75-1/-2
ビカット軟化温度, B 104 °C ISO 306
線膨張係数, 平行 90 E-6/K ISO 11359-1/-2
1.5mm厚さでの燃焼性 HB class IEC 60695-11-10
試験片の厚さ 1.5 mm -
Yellow Card 可用 はい - -
電気的特性.単位テスト基準
ISO データ
比誘電率, 1MHz 3.1 - IEC 62631-2-1
誘電正接, 1MHz 150 E-4 IEC 62631-2-1
体積抵抗率 1E13 Ohm*m IEC 62631-3-1
表面抵抗率 1E14 Ohm IEC 62631-3-2
耐電圧 30 kV/mm IEC 60243-1
耐トラッキング性 600 - IEC 60112
その他の特性.単位テスト基準
吸水率 0.6 % Sim. to ISO 62
吸湿率 0.2 % Sim. to ISO 62
密度 1040 kg/m³ ISO 1183
試験片の成形条件.単位テスト基準
ISO データ
ISO規格による成形条件 2580 - ISO ....-2
射出成形, 樹脂温度 250 °C ISO 294
射出成形, 金型温度 60 °C ISO 294
射出成形, 射出速度 200 mm/s ISO 294
射出成形, 保圧 70 MPa ISO 294
機能
 粘度せん断速度. , SINKRAL® B4 Milano, ABS, Versalis
 せん断応力-せん断速度. , SINKRAL® B4 Milano, ABS, Versalis
 せん断弾性率-温度. , SINKRAL® B4 Milano, ABS, Versalis
 応力-ひずみ. , SINKRAL® B4 Milano, ABS, Versalis
 割線弾性率−ひずみ. , SINKRAL® B4 Milano, ABS, Versalis
 pvT , SINKRAL® B4 Milano, ABS, Versalis
 DSC , SINKRAL® B4 Milano, ABS, Versalis
特殊な特性
成形加工法.
フィルム押出成形., 異形押出成形., シート押出成形., その他の押出成形., ブロー成形., 熱成形.
納入形状.
ペレット.
特殊な特性.
熱安定化.
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ., 近東/アフリカ
その他の情報
フィルム押出成形.
PREPROCESSING

Drying conditions if no venting:

    Drying temperature                80 °C

    Drying time                          2 - 4 h

    Maximum water content         0.2 %



PROCESSING

  Typical processing temperature range:

    Melt temperature           190 - 230 °C

その他の押出成形.
Other  extrusion
PREPROCESSING

Drying conditions if no venting:

    Drying temperature                80 °C

    Drying time                          2 - 4 h

    Maximum water content         0.2 %



PROCESSING

Typical processing temperature range:

    Melt temperature         190 - 230 °C

族臓遜造揃
PREPROCESSING

Drying conditions if no venting:

    Drying temperature                80 °C

    Drying time                          2 - 4 h

    Maximum water content         0.2 %



PROCESSING

Typical processing temperature range:

    Melt temperature         190 - 230 °C

促揃臓村促速揃
PREPROCESSING

Drying conditions if no venting:

    Drying temperature                80 °C

    Drying time                          2 - 4 h

    Maximum water content         0.2 %



PROCESSING

Typical processing temperature range:

    Melt temperature         190 - 230 °C

Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.