Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Treva™ GC6021-71 - CAP - Eastman Chemical Co.

Material Data Center offers the following functions for Treva™ GC6021-71:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Treva datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文

Eastman TREVA™ Renew engineering bioplastic TR6021-71 Natural is a new cellulose-based engineering bioplastic that offers both high performance and reduced environmental impact. Renew polymers enable a brand to reduce

consumption of fossil feedstock-based plastics, achieve sustainability targets without compromise, and be a fast mover in a growing market for sustainable consumer products.

TREVA is chemically resistant, dimensionally stable, flows well, is BPA-free, and has low birefringence.


Processing/Physical Characteristics単位テスト基準
ASTM数据
成形収縮率., 平行 0.008 mm/mm ASTM D 955
機械的特性単位テスト基準
ISO データ
引張弾性率 1880 MPa ISO 527
降伏応力 47 MPa ISO 527
降伏ひずみ 5 % ISO 527
破壊応力 44 MPa ISO 527
破壊ひずみ 41 % ISO 527
曲げ弾性率, 23°C 1730 MPa ISO 178
曲げ強さ 64 MPa ISO 178
ノッチ付きIzod衝撃強さ, +23°C 25 kJ/m² ISO 180/1A
ノッチ付きIzod衝撃強さ 14 kJ/m² ISO 180/1A
温度 -40 °C -
ASTM数据
降伏応力 50 MPa ASTM D 638
破壊応力 48 MPa ASTM D 638
破断伸び 22 % ASTM D 638
曲げ弾性率 1946 MPa ASTM D 790
ロックウェル硬度 R 102 - ASTM D 785
ノッチ付きIzod衝撃強さ, 1/8 in 195 J/m ASTM D 256
ノッチ付きIzod衝撃強さ, Low-Temperature 80 J/m ASTM D 256
温度 -40 °C -
熱的特性単位テスト基準
ASTM数据
DTUL @ 66 psi 114 °C ASTM D 648
DTUL @ 264 psi 100 °C ASTM D 648
ビカット軟化温度 130 °C ASTM D 1525
その他の特性.単位テスト基準
Biobased content 48 % -
吸水率, 24hr 2.2 % ASTM D 570
密度 1220 kg/m³ ASTM D 792
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 75 °C -
Pre-drying - Time 4 h -
樹脂温度 260 °C -
金型温度 85 °C -
Injection speed 30 mm/s -
Maximum residence time 4 min -
特殊な特性
成形加工法.
射出成形.
特殊な特性.
透明.
な特性
Low Birefringence
耐薬品性
General Chemical Resistance
Certifications
Contains renewable resources
アプリケーション
パッケージング
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ., 近東/アフリカ
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.