Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Tritan™ MX731 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Tritan™ MX731:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Tritan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文

Eastman Tritan™ Copolyester MX731 is an amorphous product with excellent appearance and clarity. Eastman Tritan™ Copolyester MX731 is a high flow medical grade of Eastman Tritan™ that has viscosity reductions of 40-50% relative to Eastman Tritan™ Copolyester MX711. Eastman Tritan™ Copolyester MX731 contains a mold release derived from vegetable based sources. Eastman Tritan™ Copolyester MX731 has many outstanding features that include excellent toughness, hydrolytic stability, heat resistance, chemical resistance, and melt

flowability. Eastman Tritan™ Copolyester MX731 has been formulated for medical devices. Eastman Tritan™ Copolyester MX731 has been tested for FDA/ISO 10993 and USP Class VI Biological Evaluation testing after Gamma and ETO sterilization.




Processing/Physical Characteristics単位テスト基準
ASTM数据
成形収縮率., 平行 0.006 mm/mm ASTM D 955
機械的特性単位テスト基準
ISO データ
引張弾性率 1600 MPa ISO 527
降伏応力 44 MPa ISO 527
降伏ひずみ 7 % ISO 527
破壊応力 49 MPa ISO 527
破壊ひずみ 154 % ISO 527
曲げ弾性率, 23°C 1500 MPa ISO 178
曲げ強さ 60 MPa ISO 178
ノッチ付きIzod衝撃強さ, +23°C 83 kJ/m² ISO 180/1A
ノッチ付きIzod衝撃強さ 11 kJ/m² ISO 180/1A
温度 -40 °C -
ASTM数据
引張弾性率 1575 MPa ASTM D 638
降伏応力 43 MPa ASTM D 638
破壊応力 52 MPa ASTM D 638
降伏点伸び 7 % ASTM D 638
破断伸び 210 % ASTM D 638
曲げ弾性率 1575 MPa ASTM D 790
ロックウェル硬度 R 111 - ASTM D 785
ノッチ付きIzod衝撃強さ, 1/8 in 860 J/m ASTM D 256
アイゾット衝撃試験, 1/8 in N J/m ASTM D 256
熱的特性単位テスト基準
ASTM数据
DTUL @ 66 psi 94 °C ASTM D 648
DTUL @ 264 psi 81 °C ASTM D 648
光学特性単位テスト基準
ASTM数据
ヘイズ 1 % ASTM D 1003
視感透過率 91 % ASTM D 1003
その他の特性.単位テスト基準
密度 1180 kg/m³ ASTM D 792
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 88 °C -
Pre-drying - Time 4 - 6 h -
樹脂温度 260 - 282 °C -
金型温度 38 - 66 °C -
特殊な特性
成形加工法.
射出成形.
添加剤.
離型剤.
特殊な特性.
熱安定化., 透明., 滅菌可能, エチレンオキシド滅菌(EtO), Gamma irradiation sterilization
な特性
Amorphous, Color Stability, Copolymer
耐薬品性
General Chemical Resistance, Hydrolytically Stable, Radiation Resistance
Certifications
Food contact, Food approval FDA 21 CFR, Medical Grade, Biocompatibility ISO 10993, US Pharmacopeia Class VI Approved
アプリケーション
医療の
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ., 近東/アフリカ
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.