Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultrafuse PAHT CF15 - PA*-CF15 - BASF

Material Data Center offers the following functions for Ultrafuse PAHT CF15:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Ultrafuse datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics乾燥/調湿単位テスト基準
ISO データ
メルトボリュームレイト, MVR 42.2 / * cm³/10min ISO 1133
温度 275 / * °C -
荷重 5 / * kg -
熱的特性乾燥/調湿単位テスト基準
ISO データ
溶融温度, 10゚C/min 234 / * °C ISO 11357-1/-3
ガラス転移点, 10゚C/min 70 / * °C ISO 11357-1/-2
荷重たわみ温度, 1.80 MPa 92 / * °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 145 / * °C ISO 75-1/-2
その他の特性.乾燥/調湿単位テスト基準
密度. 1230 / 1230 kg/m³ ISO 1183
3D Data乾燥/調湿単位テスト基準
Other Standards[S]
引張弾性率, flat 8390 / 5050 MPa ISO 527
引張弾性率, upright 3530 / 2460 MPa ISO 527
引張強度, flat 103 / 62.9 MPa ISO 527
引張強度, upright 18.2 / 19.1 MPa ISO 527
破壊ひずみ, flat 1.8 / 2.9 % ISO 527
破壊ひずみ, upright 0.5 / 0.8 % ISO 527
曲げ弾性率, flat 8260 / 6060 MPa ISO 178
曲げ弾性率, on-edge 7670 / 6260 MPa ISO 178
曲げ弾性率, upright 2710 / 2190 MPa ISO 178
曲げ強さ, flat 161 / 125 MPa ISO 178
曲げ強さ, on-edge 172 / 122 MPa ISO 178
曲げ強さ, upright 50.8 / 56 MPa ISO 178
シャルピー衝撃強さ, +23°C, flat 20.6 / 21.9 kJ/m² ISO 179/1eU
シャルピー衝撃強さ, +23°C, on-edge 19.3 / 20.4 kJ/m² ISO 179/1eU
シャルピー衝撃強さ, +23°C, upright 2.9 / 2.8 kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C, flat 4.8 / 5.1 kJ/m² ISO 179/1eA
ノッチ付きシャルピー衝撃強さ, +23°C, on-edge 3.9 / 5.3 kJ/m² ISO 179/1eA
ノッチ付きシャルピー衝撃強さ, +23°C, upright 1.3 / 1.6 kJ/m² ISO 179/1eA
アイゾット衝撃試験, +23°C, flat 16.4 / 16.3 kJ/m² ISO 180/1U
アイゾット衝撃試験, +23°C, on-edge 18.1 / 15.1 kJ/m² ISO 180/1U
アイゾット衝撃試験, +23°C, upright 2.9 / 4.1 kJ/m² ISO 180/1U
ノッチ付きIzod衝撃強さ, +23°C, flat 4.9 / 6.5 kJ/m² ISO 180/1A
ノッチ付きIzod衝撃強さ, +23°C, on-edge 5.1 / 5.8 kJ/m² ISO 180/1A
S: These properties are reported by the producer according standards that are different to our defaults.
特殊な特性
成形加工法.
Additive Manufacturing
納入形状.
Monofilament
特殊な特性.
熱安定化.
耐薬品性
General Chemical Resistance
領域別の利用可能性
北アメリカ., ヨーロッパ., 南・中央アメリカ.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.