Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultrafuse TPU 80A LF - TPU - BASF

Material Data Center offers the following functions for Ultrafuse TPU 80A LF:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Ultrafuse datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトボリュームレイト, MVR 82.5 cm³/10min ISO 1133
温度 210 °C -
荷重 10 kg -
機械的特性単位テスト基準
ISO データ
圧縮永久ひずみ 70℃, 24h 52 % ISO 815
耐摩耗性 56 mm³ ISO 4649
ショア硬さA 89 - ISO 7619-1
ショア硬さD 35 - ISO 7619-1
熱的特性単位テスト基準
ISO データ
ガラス転移点, 10゚C/min -44 °C ISO 11357-1/-2
その他の特性.単位テスト基準
密度. 1100 kg/m³ ISO 1183
3D Data単位テスト基準
Other Standards[S]
破壊応力, flat 35 MPa ISO 527
破壊応力, upright 7 MPa ISO 527
破壊ひずみ, flat 610 % ISO 527
破壊ひずみ, upright 230 % ISO 527
シャルピー衝撃強さ, -30°C, flat 0 kJ/m² ISO 179/1eU
シャルピー衝撃強さ, -30°C, on-edge 0 kJ/m² ISO 179/1eU
シャルピー衝撃強さ, -30°C, upright 0 kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C, flat 0 kJ/m² ISO 179/1eA
ノッチ付きシャルピー衝撃強さ, +23°C, on-edge 0 kJ/m² ISO 179/1eA
ノッチ付きシャルピー衝撃強さ, +23°C, upright 0 kJ/m² ISO 179/1eA
ノッチ付きシャルピー衝撃強さ, -30°C, flat 0 kJ/m² ISO 179/1eA
ノッチ付きシャルピー衝撃強さ, -30°C, on-edge 0 kJ/m² ISO 179/1eA
ノッチ付きシャルピー衝撃強さ, -30°C, upright 0 kJ/m² ISO 179/1eA
ノッチ付きIzod衝撃強さ, +23°C, flat 0 kJ/m² ISO 180/1A
ノッチ付きIzod衝撃強さ, +23°C, on-edge 0 kJ/m² ISO 180/1A
ノッチ付きIzod衝撃強さ, +23°C, upright 0 kJ/m² ISO 180/1A
伸び率50%時の応力, flat 5.8 MPa ISO 527
伸び率50%時の応力, upright 4.6 MPa ISO 527
伸び率100%時の応力, flat 6.9 MPa ISO 527
伸び率100%時の応力, upright 5.4 MPa ISO 527
伸び率200%時の応力, flat 11.5 MPa ISO 527
体積抵抗率, flat 2.3E10 Ohm*m IEC 62631-3-1
体積抵抗率, on-edge 1.6E10 Ohm*m IEC 62631-3-1
体積抵抗率, upright 1.6E10 Ohm*m IEC 62631-3-1
S: These properties are reported by the producer according standards that are different to our defaults.
特殊な特性
成形加工法.
Additive Manufacturing
納入形状.
Monofilament
領域別の利用可能性
北アメリカ., ヨーロッパ., 南・中央アメリカ.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.