Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAKEEP® 2000 FC30 - (PEEK+PTFE)-(CF+CD)20 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAKEEP® 2000 FC30:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestakeep datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
Carbon fiber-reinforced, graphite and PTFE-filled polyether ether ketone

VESTAKEEP® 2000 FC30 is a medium-viscosity, carbon fiber-reinforced, graphite and PTFE filled polyether ether ketone for injection molding.

The semi-crystalline polymer features superior mechanical, thermal, and chemical resistance. Parts made from VESTAKEEP® 2000 FC30 are of low flammability.

Parts made of this resin can be used for bearing bushing or gearbox parts, due to the self-lubricating effect.

VESTAKEEP® 2000 FC30 can be processed by common injection-molding machines for thermoplastics.

We recommend a melt temperature between 370°C and 380°C during the injection molding process. The mold temperature should be within a range of 160°C to 200°C, preferably 180°C. If temperatures exceed 380°C, toxic gases can be released. Adequate ventilation and protective equipment must be provided.

VESTAKEEP® 2000 FC30 is supplied as cylindrical pellets in 25 kg boxes with moisture-proof polyethylene liners.

Pigmentation may affect values.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAKEEP® 2000 FC30, please follow the general recommendations in our brochure “VESTAKEEP® PEEK Processing Guidelines“.

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM OR VISIT OUR PRODUCT AT  WWW.INDUSTRIAL.VESTAKEEP.COM
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトボリュームレイト, MVR 20 cm³/10min ISO 1133
温度 380 °C -
荷重 5 kg -
成形収縮率, 平行 0.1 % ISO 294-4, 2577
成形収縮率, 直角 0.4 % ISO 294-4, 2577
機械的特性単位テスト基準
ISO データ
引張弾性率 12600 MPa ISO 527
破壊応力 150 MPa ISO 527
破壊ひずみ 2 % ISO 527
シャルピー衝撃強さ, +23°C 40 kJ/m² ISO 179/1eU
Type of failure C - -
シャルピー衝撃強さ, -30°C 40 kJ/m² ISO 179/1eU
Type of failure C - -
ノッチ付きシャルピー衝撃強さ, +23°C 6 kJ/m² ISO 179/1eA
Type of failure C - -
ノッチ付きシャルピー衝撃強さ, -30°C 5 kJ/m² ISO 179/1eA
Type of failure C - -
熱的特性単位テスト基準
ISO データ
溶融温度, 10°C/min 340 °C ISO 11357-1/-3
荷重たわみ温度, 1.80 MPa 320 °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 337 °C ISO 75-1/-2
ビカット軟化温度, B 335 °C ISO 306
線膨張係数, 平行 20 E-6/K ISO 11359-1/-2
1.5mm厚さでの燃焼性 V-0 class IEC 60695-11-10
試験片の厚さ 1.6 mm -
酸素指数 44 % ISO 4589-1/-2
電気的特性.単位テスト基準
ISO データ
比誘電率, 100Hz 5.9 - IEC 62631-2-1
比誘電率, 1MHz 4.9 - IEC 62631-2-1
誘電正接, 100Hz 700 E-4 IEC 62631-2-1
誘電正接, 1MHz 200 E-4 IEC 62631-2-1
体積抵抗率 100000 Ohm*m IEC 62631-3-1
表面抵抗率 1000000 Ohm IEC 62631-3-2
その他の特性.単位テスト基準
吸水率 0.4 % Sim. to ISO 62
密度 1450 kg/m³ ISO 1183
特殊な特性
成形加工法.
射出成形.
納入形状.
ペレット.
耐薬品性
General Chemical Resistance
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.