Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAKEEP® Care M20 G - PEEK - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAKEEP® Care M20 G:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestakeep datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
Medium viscosity, unreinforced polyether ether ketone designed for the medical device industry

VESTAKEEP® Care is the ideal materials for the fabrication of medical devices with short time contact to human blood, tissue or bone for up to 30 days. VESTAKEEP® Care Grades have a good biocompatibility, processability and the option to pigment.

VESTAKEEP® Care M20 G is a medium viscosity, unreinforced polyether ether ketone for injection molding.

The semi-crystalline polymer features superior thermal and chemical resistance.


Biocompatibility of VESTAKEEP® Care

Biocompatiblity was tested following ISO10993-1 recommendations for a surface medical device with up to 30 days body contact.
 
The material fulfills the requirements of USP<88> class VI.
 
Tests were performed by independent, certified laboratories.

Biocompatibility tests for VESTAKEEP® Care:

 
Processing of VESTAKEEP® Care
VESTAKEEP® Care resins can be processed using all conventional melt processing techniques such as injection moulding, extrusion, and compression moulding.

VESTAKEEP® Care M20 G can be processed by common machines for thermoplastics. We recommend a melt temperature between 360°C and 380°C during the injection molding process. The mold temperature should be within a range of 160°C to 200°C, preferably 180°C.

Our technical experts would appreciate to give you support regarding the special requirements for the processing of VESTAKEEP® Care M20 G.

Delivery of VESTAKEEP® Care
VESTAKEEP® Care M20 G is supplied as granules in 25 kg boxes with moisture-proof polyethylene liners.


The results shown have been generated from a low number of production lots. Therefore, they are preliminary and not yet the result of a statistical evaluation. Therefore they must not be used to establish specifications.

The values presented are typical or average values, they do not constitute a specification. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.EVONIK.COM/MEDICAL-TECHNOLOGY 

 
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトボリュームレイト, MVR 70 cm³/10min ISO 1133
温度 380 °C -
荷重 5 kg -
成形収縮率, 平行 1.1 % ISO 294-4, 2577
成形収縮率, 直角 1.1 % ISO 294-4, 2577
機械的特性単位テスト基準
ISO データ
引張弾性率 3700 MPa ISO 527
降伏応力 100 MPa ISO 527
降伏ひずみ 5 % ISO 527
破壊呼びひずみ 40 % ISO 527
シャルピー衝撃強さ, +23°C N kJ/m² ISO 179/1eU
シャルピー衝撃強さ, -30°C N kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C 6 kJ/m² ISO 179/1eA
Type of failure C - -
ノッチ付きシャルピー衝撃強さ, -30°C 6 kJ/m² ISO 179/1eA
Type of failure C - -
熱的特性単位テスト基準
ISO データ
ビカット軟化温度, B 310 °C ISO 306
線膨張係数, 平行 60 E-6/K ISO 11359-1/-2
電気的特性.単位テスト基準
ISO データ
比誘電率, 1MHz 2.8 - IEC 62631-2-1
体積抵抗率 >1E13 Ohm*m IEC 62631-3-1
耐トラッキング性 200 - IEC 60112
その他の特性.単位テスト基準
密度 1300 kg/m³ ISO 1183
試験片の成形条件.単位テスト基準
ISO データ
射出成形, 樹脂温度 380 °C ISO 294
射出成形, 金型温度 180 °C ISO 294
射出成形, 射出速度 200 mm/s ISO 294
特殊な特性
成形加工法.
射出成形.
納入形状.
ペレット.
な特性
Thermal Stability
耐薬品性
General Chemical Resistance
Certifications
Medical Grade, Biocompatibility ISO 10993, US Pharmacopeia Class VI Approved
アプリケーション
医療の
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ., 近東/アフリカ
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.