Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAKEEP® i5 R - PEEK - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAKEEP® i5 R:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestakeep datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
Implantable grade polyether ether ketone rod stock for permanent implants

VESTAKEEP® i5 R is rod stock based on implantable grade neat polyether ether ketone resin VESTAKEEP® i5 G.

Proven Biocompatibility of VESTAKEEP® i-Grades

The extra high purity and extended quality measures make VESTAKEEP® i-grade materials an excellent choice for permanent implants.

The biocompatibility of VESTAKEEP® i5 R has been tested following ISO 10993-1 recommendations for permanent tissue/bone contact and USP Class VI.

VESTAKEEP® i5 R complies to ASTM F2026 “Standard Specification for Polyetheretherketone (PEEK) Polymers for Surgical Implant Applications”.
 
A summary of biocompatibility test results is available upon request.

Biocompatibility tests available for i5 R



Delivery of VESTAKEEP® i-Grades
VESTAKEEP® i5 R rods are available in different diameters and lengths.

Dimensions of VESTAKEEP® i5 R
Diameter Standard length*
6 to 20 mm 3000 mm
25 to 60 mm 2000 mm
70 to 100 mm 1000 mm
* Custom lengths are also available

The values presented are typical or average values, they do not constitute a specification. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.EVONIK.COM/MEDICAL-TECHNOLOGY


 
機械的特性単位テスト基準
ISO データ
引張弾性率 3900 MPa ISO 527
降伏応力 105 MPa ISO 527
降伏ひずみ 4.6 % ISO 527
破壊呼びひずみ 20 % ISO 527
熱的特性単位テスト基準
ISO データ
溶融温度, 10°C/min 340 °C ISO 11357-1/-3
荷重たわみ温度, 1.80 MPa 155 °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 205 °C ISO 75-1/-2
電気的特性.単位テスト基準
ISO データ
比誘電率, 1MHz 2.8 - IEC 62631-2-1
その他の特性.単位テスト基準
吸水率 0.4 % Sim. to ISO 62
吸湿率 0.12 % Sim. to ISO 62
密度 1300 kg/m³ ISO 1183
特殊な特性
納入形状.
Semifinished product
Certifications
Medical Grade, Biocompatibility ISO 10993, US Pharmacopeia Class VI Approved
アプリケーション
医療の
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ., 近東/アフリカ
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.