Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® DX9325 BK E70352 - PA612-GF40 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® DX9325 BK E70352:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
Heat-stabilized, glass fiber-reinforced, PA 612 compound for plastic-EPDM-rubber bonds

VESTAMID® DX9325 BK E70352 is a glass fiber-reinforced, PA 612 molding compound. The material contains about 40% glass fiber, an ageing protective agent and processing aid for a fast and even form filling. VESTAMID® DX9325 BK E70352 is especially suitable for the production of plastic and rubber composites. 

Parts of VESTAMID® DX9325 BK E70352 can be co-vulcanized with EPDM-rubbers without using any adhesives or adhesion promoters ("direct-bonding to rubber"). Because of its semi-crystalline morphology VESTAMID® DX9325 BK E70352 provides an excellent chemical resistance, e. g., against greases, oils, fuels and hydraulic fluids.

VESTAMID® DX9325 BK E70352 is supplied as cylindrical pellets ready for processing in moisture-proof bags.

Very important are predrying conditions. The material has to be handle as plasticized PA 612. The drying temperature should be not more than 80°C and the drying time at this temperature not more than 4h.
 
Pigmentation may affect values.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

The values presented are typical or average values, they do not constitute a specification.

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM
Processing/Physical Characteristics乾燥/調湿単位テスト基準
ISO データ
成形収縮率, 平行 0.2 / * % ISO 294-4, 2577
成形収縮率, 直角 0.7 / * % ISO 294-4, 2577
機械的特性乾燥/調湿単位テスト基準
ISO データ
引張弾性率 10300 / - MPa ISO 527
破壊応力 160 / - MPa ISO 527
破壊ひずみ 4.4 / - % ISO 527
シャルピー衝撃強さ, +23°C 100 / - kJ/m² ISO 179/1eU
Type of failure C / - - -
シャルピー衝撃強さ, -30°C 104 / - kJ/m² ISO 179/1eU
Type of failure C / - - -
ノッチ付きシャルピー衝撃強さ, +23°C 18 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
ノッチ付きシャルピー衝撃強さ, -30°C 16 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
熱的特性乾燥/調湿単位テスト基準
ISO データ
荷重たわみ温度, 1.80 MPa 200 / * °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 215 / * °C ISO 75-1/-2
その他の特性.乾燥/調湿単位テスト基準
密度 1410 / - kg/m³ ISO 1183
試験片の成形条件.単位テスト基準
ISO データ
射出成形, 樹脂温度 260 °C ISO 294
射出成形, 金型温度 80 °C ISO 294
射出成形, 射出速度 200 mm/s ISO 294
特殊な特性
成形加工法.
射出成形.
納入形状.
ペレット., 黒
添加剤.
離型剤.
特殊な特性.
光安定化., 熱安定化.
な特性
Good Adhesion
耐薬品性
General Chemical Resistance, Grease Resistance, Oil Resistance
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ., 近東/アフリカ
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.