Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® Terra HS1851 - PA610-GF20 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® Terra HS1851:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
Medium viscosity, glass fiber–reinforced, easily demoldable, heat-stabilized polyamide 610 compound for efficient injection molding

VESTAMID® Terra HS1851 is a glass fiber-reinforced, heat-stabilized, medium-viscosity PA 610 compound for injection molding application. The material contains about 20% glass fibers, an ageing protective agent and processing aid for a fast and even form filling.

The carbonamide groups (-CO-NH-) of the polyamides form hydrogen bridge bonds between the chains of the macromolecules, thereby substantially promoting crystallinity and increasing their strength, melting point, resistance to chemicals and even water absorption. This is characteristic of all semi-crystalline polyamides.

Because of its semi-crystalline morphology VESTAMID® Terra HS1851 provides a high impact strength, excellent chemical resistance (e.g. against greases, oils, alkalis and saline solutions), a low coefficient of friction and high abrasion resistance.
 

VESTAMID® Terra HS1851 is supplied as cylindrical granules, ready for processing, in moisture-proof bags.

 

VESTAMID® Terra is a group of new polyamides, the monomers for which are based entirely or partly on renewable raw materials.
 

VESTAMID® Terra HS is the polycondensation product of 1,6-hexamethylene diamine (H) and 1,10-decanedioic acid (sebacic acid—S). Because sebacic acid is derived from castor oil, VESTAMID® Terra HS is a material that is partly based on bio-based and renewable resources.
 

The use of colorants may affect property values. 

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

The values presented are typical or average values, they do not constitute a specification.

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM OR VISIT OUR PRODUCT AT  WWW.VESTAMID.TERRA.COM
Processing/Physical Characteristics乾燥/調湿単位テスト基準
ISO データ
メルトボリュームレイト, MVR 21 / * cm³/10min ISO 1133
温度 250 / * °C -
荷重 5 / * kg -
成形収縮率, 平行 0.4 / * % ISO 294-4, 2577
成形収縮率, 直角 0.7 / * % ISO 294-4, 2577
機械的特性乾燥/調湿単位テスト基準
ISO データ
引張弾性率 6000 / - MPa ISO 527
破壊応力 131 / - MPa ISO 527
破壊ひずみ 3.8 / - % ISO 527
シャルピー衝撃強さ, +23°C 86 / - kJ/m² ISO 179/1eU
Type of failure C / - - -
シャルピー衝撃強さ, -30°C 78 / - kJ/m² ISO 179/1eU
Type of failure C / - - -
ノッチ付きシャルピー衝撃強さ, +23°C 11 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
ノッチ付きシャルピー衝撃強さ, -30°C 8.9 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
熱的特性乾燥/調湿単位テスト基準
ISO データ
溶融温度, 10°C/min 223 / * °C ISO 11357-1/-3
ガラス転移点, 10°C/min 49 / * °C ISO 11357-1/-2
荷重たわみ温度, 1.80 MPa 204 / * °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 222 / * °C ISO 75-1/-2
ビカット軟化温度, B 219 / * °C ISO 306
線膨張係数, 平行 26 / * E-6/K ISO 11359-1/-2
線膨張係数, 直角 124 / * E-6/K ISO 11359-1/-2
その他の特性.乾燥/調湿単位テスト基準
吸水率 2.6 / * % Sim. to ISO 62
密度 1220 / - kg/m³ ISO 1183
試験片の成形条件.単位テスト基準
ISO データ
射出成形, 樹脂温度 260 °C ISO 294
射出成形, 金型温度 80 °C ISO 294
射出成形, 射出速度 200 mm/s ISO 294
特殊な特性
成形加工法.
射出成形.
納入形状.
ペレット.
特殊な特性.
高耐衝撃及び耐衝撃改良., 熱安定化.
な特性
Tribologic Grade
耐薬品性
Alkali Resistance, General Chemical Resistance, Grease Resistance, Oil Resistance
Certifications
Contains renewable resources
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ., 近東/アフリカ
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.