Processing/Physical Characteristics | 値 | 単位 | テスト基準 |
ASTM数据 |
メルトフローレイト, MFI |
3.7 |
g/10min |
ASTM D 1238 |
温度 |
190 |
°C |
- |
荷重 |
2.16 |
kg |
- |
熱的特性 | 値 | 単位 | テスト基準 |
Other Standards[S] |
溶融温度 |
106 |
°C |
ExxonMobil Method |
S: | These properties are reported by the producer according standards that are different to our defaults. |
光学特性 | 値 | 単位 | テスト基準 |
ASTM数据 |
光沢度 |
89 |
- |
ASTM D 2457 |
Other Standards[S] |
ヘイズ |
0.4 |
% |
ExxonMobil Method |
S: | These properties are reported by the producer according standards that are different to our defaults. |
その他の特性. | 値 | 単位 | テスト基準 |
Other Standards[S] |
密度 |
889 |
kg/m³ |
ExxonMobil Method |
S: | These properties are reported by the producer according standards that are different to our defaults. |
機械的特性(ィルム) | 値 | 単位 | テスト基準 |
ASTM Data |
押出成形のタイプ |
cast |
- |
- |
試験片の厚さ |
0.0254 |
mm |
- |
Other Standards[S] |
降伏応力, 平行 |
15.2 |
MPa |
ExxonMobil Method |
降伏応力, 直角 |
13.1 |
MPa |
ExxonMobil Method |
破壊応力, 平行 |
62.7 |
MPa |
ExxonMobil Method |
破壊応力, 直角 |
35.9 |
MPa |
ExxonMobil Method |
破断伸び, 平行 |
440 |
% |
ExxonMobil Method |
破断伸び, 直角 |
790 |
% |
ExxonMobil Method |
S: | These properties are reported by the producer according standards that are different to our defaults. |
特殊な特性
成形加工法.
フィルム押出成形.
な特性
Copolymer
Certifications
RoHS
アプリケーション
パッケージング
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ., 近東/アフリカ
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com