Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Bergamid AB" in Material Data Center leads to the following information:

Tradename: Bergamid AB
Family: PA666
Producer: Avient Corporation
8 hits in the material database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Polymer
BERGAMID® AB700UF PA666
Bergamid™ AB70 G40 H UF Natural PA666-GF40
Bergamid™ AB70 MI30 GR012 PA66-MX30
Bergamid™ AB700 UF BK138 PA666
Bergamid™ AB700 UF SO PA666
BERGAMID® AB700G20U PA666-GF20
BERGAMID® AB70MI10U PA666-MD10
BERGAMID® AB70MI20UF PA666-MD20

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.