Bestnyl - PA6, PA66 - Grupo Triesa

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Bestnyl" in Material Data Center leads to the following information:

Tradename: Bestnyl
Family: PA6, PA66
Producer: Grupo Triesa
73 hits in the material database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Polymer
BESTNYL ABP70U /02 (PA*+ABS)
BESTNYL PPA 60E (PA*+PP)
BESTNYL SC00VI01AWX (PA6+PA66)
BESTNYL SC00VI02AH15 (PA6+PA66)-MX30
BESTNYL SC30VI02BMU (PA6+PA66)-GF30
BESTNYL SE00VI01A PA66
BESTNYL SE00VI01AHQ03 PA66-Z5
BESTNYL SE00VI01AM PA66
BESTNYL SE00VI01AM-1 PA66
BESTNYL SE00VI01AS08 PA66
BESTNYL SE00VI01AT (PA66+PTFE)
BESTNYL SE00VI02AH PA66
BESTNYL SE00VI02AM PA66
BESTNYL SE10VI01A PA66-GF10
BESTNYL SE10VI02AU PA66-GF10
BESTNYL SE15VI01A PA66-GF15
BESTNYL SE15VI02AS08 PA66-GF15
BESTNYL SE15VI02AS16 PA66-(GF+MX)40
BESTNYL SE15VI02AU PA66-GF15
BESTNYL SE15VI02AX PA66-GF15
BESTNYL SE20VI01AHQ03 PA66-(GF+Z)25
BESTNYL SE25VI01A PA66-GF25
BESTNYL SE25VI01AWX PA66-GF25
BESTNYL SE25VI01AX-1 PA66-GF25
BESTNYL SE25VI02A PA66-GF25
BESTNYL SE25VI02AHC PA66-GF25
BESTNYL SE25VI02AX PA66-GF25
BESTNYL SE30CB02AH PA66-CF30
BESTNYL SE30VI01AH PA66-GF30
BESTNYL SE30VI01AT (PA66+PTFE)-GF30
BESTNYL SE30VI02AH PA66-GF30
BESTNYL SE30VI02AS08 PA66-GF30
BESTNYL SE30VI02AWXL PA66-GF30
BESTNYL SE30VI11AHD PA66-GF30
BESTNYL SE35VI01AH PA66-GF35
BESTNYL SE35VI01AX PA66-GF35
BESTNYL SE35VI02AU PA66-GF35
BESTNYL SE35VI02AX PA66-GF35
BESTNYL SE43VI11AH-1 PA66-GF43
BESTNYL SE50VI02AH PA66-GF50
BESTNYL SI00VI01BE PA6
BESTNYL SI00VI01BM PA6
BESTNYL SI00VI01BN PA6
BESTNYL SI00VI01BN-1 PA6
BESTNYL SI00VI01BS08 PA6
BESTNYL SI00VI01BWX PA6
BESTNYL SI00VI02B PA6
BESTNYL SI00VI02BEHX PA6
BESTNYL SI00VI02BH14 PA6-MX20
BESTNYL SI00VI02BHC PA6
BESTNYL SI00VI02BM PA6
BESTNYL SI00VI02BU PA6
BESTNYL SI00VI02BX PA6
BESTNYL SI00VI12BEWX PA6
BESTNYL SI00VI12BWX PA6
BESTNYL SI15VI01A PA6-GF15
BESTNYL SI15VI01BH16 PA6-(GF+MX)40
BESTNYL SI15VI02AU PA6-GF15
BESTNYL SI15VI02BX PA6-GF15
BESTNYL SI20CB01BH PA6-CF20
BESTNYL SI20VI01AHQ03 PA6-(GF+Z)25
BESTNYL SI20VI02AU PA6-GF20
BESTNYL SI25VI01A PA6-GF25
BESTNYL SI25VI01BX PA6-GF25
BESTNYL SI30VI01A PA6-GF30
BESTNYL SI30VI01BM PA6-GF30
BESTNYL SI30VI02ANU PA6-GF30
BESTNYL SI30VI02BHF PA6-(GF+GX)30
BESTNYL SI30VI02BNH PA6-GF30
BESTNYL SI30VI02BWX PA6-GF30
BESTNYL SI30VI02BX PA6-GF30
BESTNYL SI50VI01BHF PA6-(GF+GX)50
BESTNYL SI50VI02ANU PA6-GF50

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.