Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Bio-Flex® F 2120 - PLA... - FKuR Kunststoff GmbH

Material Data Center offers the following functions for Bio-Flex® F 2120:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Bio-Flex datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
more information can be found in the following table
Rilsamid® Chemical Resistance
Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 흐름성, MFI 5.5 g/10min ISO 1133
온도 190 °C -
负荷 2.16 kg -
열적 특성단위시험규격
ISO 데이터
녹는점, 10°C/min 155 °C ISO 11357-1/-3
기타 특성단위시험규격
밀도 1410 kg/m³ ISO 1183
기계적 성질 (필름) 단위시험규격
ISO 데이터
인장탄성률, 평행 710 MPa ISO 527-3
인장탄성률, 수직 570 MPa ISO 527-3
항복시의 변형율, parallel 4 % ISO 527-3
항복시의 변형율, 수직 5.5 % ISO 527-3
파단시 강도, 평행 27 MPa ISO 527-3
파단시 강도, 수직 22 MPa ISO 527-3
최대변형율, 평행 320 % ISO 527-3
최대변형율, 수직 330 % ISO 527-3
압출 유형 blown - -
시편두께 0.03 mm -
Processing Recommendation Extrusion단위시험규격
Type of extrusion blown - -
Pre-drying - Temperature 60 °C -
Pre-drying - Time 2 - 4 h -
용융수지온도 190 °C -
Feed temperature 40 °C -
Zone 1 150 °C -
Zone 2 160 °C -
Zone 3 160 °C -
Zone 4 170 °C -
Nozzle temperature 170 °C -
특징
생산 공정
Blown Film Extrusion, 필름 압출
인도 유형
펠렛 (입자,알갱이), 화이트
Certifications
Contains renewable resources, Biodegradable, Food contact, 퇴비화 가능 ISO 13432 (생산자), 퇴비화 가능 GreenPla (생산자)
응용
포장, 장난감
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬, 짱쨌쨈, 쩐횈쩍횄쩐횈 횇횂횈챵쩐챌 횁철쩔짧, 쨀짼쨘횓 쨔횞 횁횩쩐횙 쩐횈쨍횧쨍짰횆짬, 쨉쩔쩐챌 쨔횞 쩐횈횉횁쨍짰횆짬 짹횢쩔짧
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.