Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Cadence™ GS3 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Cadence™ GS3:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Cadence datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서

Eastman Cadence™ GS3 is a clear copolyester resin specifically for calendered film applications including

decorative laminates, general purpose packaging, transaction and identification cards, and protective films. It has

enhanced processing ease and higher melt strength compared to Cadence™ GS2.

Film producers looking to replace PVC and other materials of concern choose Cadence™ for its ease of processing,

low-temperature toughness, and the ability to be downgauged – all of which help reduce cost. It has a wide

calendering and thermoforming window, which enables Cadence™ to be used on most existing calendering lines

and thermoforming equipment with little or no modification. Eastman Cadence™ resins require no pre-drying or

additional stabilizers.

열적 특성단위시험규격
ASTM 데이터
열팽창 계수, 평행 75.2 E-6/K ASTM D 696
DTUL @ 66 psi 69 °C ASTM D 648
DTUL @ 264 psi 62 °C ASTM D 648
유리 전이 온도 80 °C ASTM E 1356
비카트 연화 온도 81 °C ASTM D 1525
산소지수 24.2 % ASTM D 2863
전기적 특성단위시험규격
ASTM 데이터
전기 압력, 단기간의 15.1 kV/mm ASTM D 149
소산 인자, 1 MHz 0.019 - ASTM D 150
상대 유전율, 1 MHz 2.43 - ASTM D 150
표면 저항 1.28E16 Ohm ASTM D 257
부피 저항 7.05E16 Ohm*cm ASTM D 257
아크 저항 135 s ASTM D 495
기타 특성단위시험규격
물에서의 흡수성, 24hr 0.15 % ASTM D 570
밀도 1280 kg/m³ ASTM D 792
특징
생산 공정
캘린더링, 열성형
특성
Low Emission, Melt Strength, Scratch Resistant, Copolymer
Certifications
Food contact, Food approval FDA 21 CFR
응용
건물 건설, 포장
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬, 짱쨌쨈, 쩐횈쩍횄쩐횈 횇횂횈챵쩐챌 횁철쩔짧, 쨀짼쨘횓 쨔횞 횁횩쩐횙 쩐횈쨍횧쨍짰횆짬, 쨉쩔쩐챌 쨔횞 쩐횈횉횁쨍짰횆짬 짹횢쩔짧
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.