Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of CALIBRE™ 5201-8 - PC-GX20 - Trinseo

Material Data Center offers the following functions for CALIBRE™ 5201-8:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Calibre datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 흐름성, MFI 8 g/10min ISO 1133
온도 300 °C -
负荷 1.2 kg -
성형 수축률, 평행 0.3 % ISO 294-4, 2577
ASTM 데이터
용융 흐름성, MFI 8 g/10min ASTM D 1238
온도 300 °C -
하중 1.2 kg -
성형 수축률, 평행 0.003 mm/mm ASTM D 955
기계적 특성단위시험규격
ISO 데이터
인장탄성률 5170 MPa ISO 527
항복강도 83 MPa ISO 527
항복변형률 2.6 % ISO 527
파단시 강도 83 MPa ISO 527
파단시 신율 3 % ISO 527
굴곡 계수, 23°C 4820 MPa ISO 178
아이조드 충격은 노치, +23°C 110 kJ/m² ISO 180/1A
ASTM 데이터
인장탄성률 5171 MPa ASTM D 638
항복강도 82.7 MPa ASTM D 638
파단시 강도 82.7 MPa ASTM D 638
항복변형률 2.6 % ASTM D 638
파단시 신율 3 % ASTM D 638
굴곡 계수 4826 MPa ASTM D 790
굴곡 강도 148 MPa ASTM D 790
로크웰 경도 R 122 - ASTM D 785
아이조드 충격은 노치, 1/8 in 107 J/m ASTM D 256
열적 특성단위시험규격
ISO 데이터
하중하에서의 변형온도, 1.80 MPa 138 °C ISO 75-1/-2
비카트 연화 온도, B 158 °C ISO 306
1.5mm 평균두께에서의 난연성 V-2 class IEC 60695-11-10
테스트 두께 1.6 mm -
두께 H인 제품의 난연성 V-0 class IEC 60695-11-10
테스트 두께 3.0 mm -
ASTM 데이터
UL94 난연성 V-2 - UL 94
테스트 두께 1.59 mm -
DTUL @ 264 psi 138 °C ASTM D 648
비카트 연화 온도 159 °C ASTM D 1525
기타 특성단위시험규격
밀도 1360 kg/m³ ISO 1183
밀도 1360 kg/m³ ASTM D 792
특징
부가물
이형제
응용
전기 및 전자 , 의료
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬, 쨀짼쨘횓 쨔횞 횁횩쩐횙 쩐횈쨍횧쨍짰횆짬
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.