Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of CELSTRAN® PP-GF50-0455 P10/10 - PP-GLF50 - Celanese

Material Data Center offers the following functions for CELSTRAN® PP-GF50-0455 P10/10:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Celstran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
Material code according to ISO 1043-1: PP Heat and light stabilized polypropylene reinforced with 50 weight percent long glass fibers. Black. The product has low emissions. The fibers are chemically coupled to the polypropylene matrix. The pellets are cylindrical and normally as well as the embedded fibers 11 mm long. Parts molded of CELSTRAN have outstanding mechanical properties such as high strength and stiffness combined with high heat deflection. The notched impact strength is increased at elevated and low temperatures due to the fiber skeleton built in the parts. The long fiber reinforcement reduces creep significantly. The very isotropic shrinkage in the molded parts minimizes the warpage. Complex parts can be manufactured with high reproducibility by injection molding. Application field: Functional/structural parts for automotive

Flammability at thickness h (1 mm)HB-
기계적 특성단위시험규격
ISO 데이터
인장탄성률 11600 MPa ISO 527
파단시 강도 140 MPa ISO 527
파단시 신율 1.8 % ISO 527
챠피 충격 강도 , +23°C 60 kJ/m² ISO 179/1eU
챠피 충격 강도, -30°C 58 kJ/m² ISO 179/1eU
챠피 노치드 충격 강도, +23°C 32 kJ/m² ISO 179/1eA
챠피 노치드 충격 강도, -30°C 33 kJ/m² ISO 179/1eA
열적 특성단위시험규격
ISO 데이터
녹는점, 10°C/min 165 °C ISO 11357-1/-3
하중하에서의 변형온도, 1.80 MPa 158 °C ISO 75-1/-2
하중하에서의 변형온도, 8.00 MPa 138 °C ISO 75-1/-2
두께 H인 제품의 난연성 HB class IEC 60695-11-10
테스트 두께 1.0 mm -
기타 특성단위시험규격
밀도 1340 kg/m³ ISO 1183
Processing Recommendation Injection Molding단위시험규격
Pre-drying - Temperature 94 °C -
Pre-drying - Time 2 h -
용융수지온도 260 - 290 °C -
성형온도 40 - 70 °C -
도표
응력-신율 , CELSTRAN® PP-GF50-0455 P10/10, PP-GLF50, Celanese
시컨트탄성율-신율 , CELSTRAN® PP-GF50-0455 P10/10, PP-GLF50, Celanese
특징
생산 공정
사출 성형, 외형 압출, 시트 압출, 기타 압출, 코팅, 중공 성형, 트랜스퍼 성형
인도 유형
펠렛 (입자,알갱이), 검정
특별 특성
가시광선 안정성, U.V. 안정성 또는 기후 안정성, 열안정성
특성
Chemically Coupled Reinforcement, Creep Resistance, Long fiber reinforced, Low Emission, Low Warpage
응용
자동차의
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬, 짱쨌쨈, 쩐횈쩍횄쩐횈 횇횂횈챵쩐챌 횁철쩔짧
기타 정보
사E성
PP&PE drying requirements: 2 hrs. @94° C.
A dehumidifier or desiccant dryer is recommended.
Celstran can be processed on a standard injection molding unit.
A general purpose metering screw is recommended with a zone
distribution of 40% feed, 40% transition, and 20% metering.
A free flowing check ring assembly is recommended.

Melt Temp: 260-290°C.
Mold Temp: 40- 70°C.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.