Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of CELSTRAN® PA66-GF50-0111P10/11 - PA666-GLF50 - Celanese

Material Data Center offers the following functions for CELSTRAN® PA66-GF50-0111P10/11:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Celstran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
Material code according to ISO 1043-1: PA66 Nylon 66/6 Copolymer reinforced by 50 weight percent long glass fibers. The pellets are cylindrical and normally as well as the embedded fibers 10 mm long. Parts molded of CELSTRAN have outstanding mechanical properties such as high strength and stiffness combined with high heat deflection. The notched impact strength is increased at elevated and low temperatures due to the fiber skeleton built in the parts. The long fiber reinforcement reduces creep significantly. The very isotropic shrinkage in the molded parts minimizes the warpage. Complex parts can be manufactured with high reproducibility by injection molding. Can be used for substituting die cast metal with the advantage of Weight reduction, no corrosion problems, no post treatment.

Flammability at thickness h (1.5 mm)HBUL recognition (h)
기계적 특성건조/응축단위시험규격
ISO 데이터
인장탄성률 16500 / 11600 MPa ISO 527
파단시 강도 275 / 180 MPa ISO 527
파단시 신율 2.2 / 2.5 % ISO 527
챠피 충격 강도 , +23°C 100 / 50 kJ/m² ISO 179/1eU
챠피 충격 강도, -30°C 80 / - kJ/m² ISO 179/1eU
챠피 노치드 충격 강도, +23°C 40 / 36 kJ/m² ISO 179/1eA
챠피 노치드 충격 강도, -30°C 42 / - kJ/m² ISO 179/1eA
열적 특성건조/응축단위시험규격
ISO 데이터
녹는점, 10°C/min 240 / * °C ISO 11357-1/-3
하중하에서의 변형온도, 1.80 MPa 235 / * °C ISO 75-1/-2
하중하에서의 변형온도, 8.00 MPa 220 / * °C ISO 75-1/-2
두께 H인 제품의 난연성 HB / * class IEC 60695-11-10
테스트 두께 1.5 / * mm -
Yellow Card 유효한 예 / * - -
기타 특성건조/응축단위시험규격
조건에서의 흡습성 1 / * % ISO 62와 유사
밀도 - / 1560 kg/m³ ISO 1183
Processing Recommendation Injection Molding단위시험규격
Pre-drying - Temperature 80 °C -
Pre-drying - Time 4 h -
용융수지온도 310 - 325 °C -
성형온도 90 - 120 °C -
특징
생산 공정
사출 성형
인도 유형
펠렛 (입자,알갱이)
특성
Creep Resistance, Long fiber reinforced, Low Warpage, Copolymer
지역별 검색
기타 정보
사E성
It is recommended to dry in a dehumidifying dryer: 4 hours at 80 °C

During the processing of CELSTRAN it is important to watch and
control melt shear, for excessive shear reduces fiber length and
mechanical performance as well.

Processing recommendation:

- Conventional 3 zone screw, screw diameter minimum 40 mm
- Design flow channels for low melt shear
- Back pressure and screw rotation to realize a continous
plastification performance and thus a homogeneous melt.
- Apply higher temperature settings than for short fiber compounds

Melt temperature (in the srew anteroom) 310-325 °C
Mold surface temperature 90-120 °C
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.