Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Clyrell EC140R - PP - LyondellBasell Industries

Material Data Center offers the following functions for Clyrell EC140R:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Clyrell datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 부피 - 흐름 속도, MVR 40.5 cm³/10min ISO 1133
온도 230 °C -
하중 2.16 kg -
용융 흐름성, MFI 30 g/10min ISO 1133
온도 230 °C -
负荷 2.16 kg -
ASTM 데이터
용융 흐름성, MFI 30 g/10min ASTM D 1238
온도 230 °C -
하중 2.16 kg -
기계적 특성단위시험규격
ISO 데이터
인장탄성률 850 MPa ISO 527
항복강도 20 MPa ISO 527
항복변형률 18 % ISO 527
파단시 신율 >50 % ISO 527
챠피 노치드 충격 강도, +23°C 20 kJ/m² ISO 179/1eA
Ball indentation hardness 28 MPa ISO 2039-1
열적 특성단위시험규격
ISO 데이터
하중하에서의 변형온도, 0.45 MPa 60 °C ISO 75-1/-2
비카트 연화 온도, A 114 °C ISO 306
비카트 연화 온도, B 52 °C ISO 306
광학 특성단위시험규격
ASTM 데이터
탁도 20 % ASTM D 1003
기타 특성단위시험규격
밀도 900 kg/m³ ISO 1183
밀도 902 kg/m³ ASTM D 792
특징
생산 공정
사출 성형
특별 특성
고충격 또는 고충격 보강, 투명도
특성
Blush Resistance/Low Crease Whitening, Copolymer, Random Copolymer
Certifications
Food contact, Food approval 1935/2004/EC, Food approval 10/2011, Food approval FDA 21 CFR
응용
스포츠 장비
지역별 검색
짱쨌쨈, 쩐횈쩍횄쩐횈 횇횂횈챵쩐챌 횁철쩔짧, 쨉쩔쩐챌 쨔횞 쩐횈횉횁쨍짰횆짬 짹횢쩔짧
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.