Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of ecovio® F2224 - (PBAT+PLA) - BASF

Material Data Center offers the following functions for ecovio® F2224:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Ecovio datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 부피 - 흐름 속도, MVR 4.75 cm³/10min ISO 1133
온도 190 °C -
하중 5 kg -
광학 특성단위시험규격
ASTM 데이터
탁도 85 % ASTM D 1003
기타 특성단위시험규격
밀도 1250 kg/m³ ISO 1183
Bulk density 740 kg/m³ -
기계적 성질 (필름) 단위시험규격
ISO 데이터
인장탄성률, 평행 1100 MPa ISO 527-3
인장탄성률, 수직 600 MPa ISO 527-3
최대강도, parallel 47 MPa ISO 527-3
최대강도, 평행 40 MPa ISO 527-3
최대변형율, 평행 440 % ISO 527-3
최대변형율, 수직 350 % ISO 527-3
엘멘도프 전단강도, 평행 0.28 N ISO 6383-2
엘멘도프 전단강도, 수직 0.23 N ISO 6383-2
압출 유형 blown - -
시편두께 0.05 mm -
특징
생산 공정
Blown Film Extrusion
인도 유형
펠렛 (입자,알갱이)
특성
Low Odor, Melt Strength, Thermal Stability, Weldable
Certifications
Contains renewable resources, Biodegradable, Food contact, 퇴비화 가능 ISO 13432 (생산자), 퇴비화 가능 ASTM D6400 (생산자), 퇴비화 가능 ISO 13432 (증명서), 퇴비화 가능 ASTM D6400 (증명서)
응용
포장
지역별 검색
짱쨌쨈
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.