Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Edgetek" in Material Data Center leads to the following information:

Tradename: Edgetek
Family: PS
Producer: Avient Corporation
191 hits in the material database
1 hits in the literature database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Polymer
Edgetek sPS® QT-30GF/000 (PS-SY)-GF30
Edgetek™ 5209 Black 30 A 1 POM
Edgetek™ AM-35GF/000 FR NH PPA-GF35
Edgetek™ AS-000/000 AS BLACK ABS
Edgetek™ AS-000/000 AS colored UV MABS
Edgetek™ AS-000/000 AS NC505 ABS
Edgetek™ AS-000/000 AS UV ABS
Edgetek™ AS-10GF/000 BLACK ABS-GF10
Edgetek™ AS-10GF/000 FR V0 BLACK ABS-GF10
Edgetek™ AS-10GF/000 NATURAL ABS-GF10
Edgetek™ AS/018 White ABS
Edgetek™ AT-000/000 BK022 POM
Edgetek™ AT-000/000 GREY VN-3581 POM
Edgetek™ AT-000/000 HI 10 Natural POM
Edgetek™ AT-000/000 NC707 POM
Edgetek™ AT-1000 POM-GF10
Edgetek™ AT-10GF/000 BLACK POM-GF10
Edgetek™ AT-10GF/000 NC702 POM-GF10
Edgetek™ AT-15GB/000 BK023 POM-GB15
Edgetek™ AT-15GB/000 BLACK POM-GB15
Edgetek™ AT-15GF/000 BLACK POM-GF15
Edgetek™ AT-15GF/000 NC702 POM-GF15
Edgetek™ AT-20GB/000 BK017 POM-GB20
Edgetek™ AT-20GF/000 BLACK POM-GF20
Edgetek™ AT-20GF/000 NC004 POM-GF20
Edgetek™ AT-25CF/000 BK001 POM-CF25
Edgetek™ AT-25GB/000 NATURAL POM-GB25
Edgetek™ AT-25GF/000 BK002 POM-GF25
Edgetek™ AT-25GF/000 NC001 POM-GF25
Edgetek™ AT-30GB/000 BK006 POM-GB30
Edgetek™ AT-30GF/000 BK004 POM-GF30
Edgetek™ AT-30GF/000 BLACK POM-GF30
Edgetek™ AT-30GF/000 NC005 S-ROHS POM-GF30
Edgetek™ COC BLEND-15GF Natural COC-GF15
Edgetek™ CY1000 G20 BK001 (PC+ABS)-GF20
Edgetek™ CY1000 GR188 (PC+ABS)
Edgetek™ CY1000 UV FR V0 BL077 (PC+ABS)
Edgetek™ CY1000 UV GR112 (PC+ABS)
Edgetek™ CY1000 UV NHFR V0 GR723 (PC+ABS)
Edgetek™ CY1000-10GF/000 D NC704 (PC+ABS)-GF10
Edgetek™ CY1000-10GF/000 FR V0 NC702 (PC+ABS)-GF10
Edgetek™ CY1000-20CF/000 BK001 (PC+ABS)-CF20
Edgetek™ CY1000-20GF/000 BK005 (PC+ABS)-GF20
Edgetek™ CY3000 AS BK (PC+ASA)
Edgetek™ CY3000 NC007 (PC+ASA)
Edgetek™ CY4000 BK006 (PC+PBT)
Edgetek™ CY4000 L BK025 (PC+PBT)
Edgetek™ CY4000 NC002 (PC+PBT)
Edgetek™ CY4000 T NC706 (PC+PBT)
Edgetek™ CY4000 UV YE703 (PC+PBT)
Edgetek™ CY4000-15GF/000 NC (PC+PBT)-GF15
Edgetek™ CY4000-30GF/000 FR V0 GR703 (PC+PBT)-GF30
Edgetek™ CY4000-65 NC015 (PC+PBT)
Edgetek™ CY8000-20GF/000 NC003 (PBT+ASA)-GF20
Edgetek™ EM01042076BG PC
Edgetek™ ES-30GF/000 Black PESU-GF30
Edgetek™ ET3200-0040 RS Black PC-GF
Edgetek™ ET3200-8001 LG PC
Edgetek™ ET3200-8086 RS Black PC
Edgetek™ ET3200-8093 FR Black PC
Edgetek™ ET3300-0030 RS White PBT
Edgetek™ ET3300-5007 Natural FD PBT
Edgetek™ ET3300-8008 FR Black PBT
Edgetek™ ET3300-8029 RS NC701 PBT
Edgetek™ ET3500-5001 (ASA+PC)
Edgetek™ ET3500-5001 colored (ASA+PC)
Edgetek™ ET3500-5002 BK (ASA+PC)-GF12
Edgetek™ ET3500-5003 (ASA+PC)
Edgetek™ ET5200-5014 NC FD PP
Edgetek™ ET6000-5008 NHFR BLACK VN-3901 PA6
Edgetek™ ET6000-5019 HI BLACK PA6
Edgetek™ ET6620-0020 FRV0 PA66
Edgetek™ ET7300-0004 Aluminum ABS
Edgetek™ ET7400-5005 WHITE VN 3926 (PS-HI)
Edgetek™ ET9200-5006 FD NATURAL PPS
Edgetek™ ET9700-5012 NHFR Natural PPA-GF15
Edgetek™ MP-10GF/000 BLACK (PPE+PS)-GF10
Edgetek™ MP-20GF/000 BK088 (PPE+PS)-GF20
Edgetek™ MP-30GF/000 BLACK (PPE+PS)-GF30
Edgetek™ NJ-30GF/000 Natural PA12
Edgetek™ NL-20GF/000 BLACK PA612-GF20
Edgetek™ NN-20CF/000 BLACK PA66-CF20
Edgetek™ NN-20CF/15T BK008 (PA66+PTFE)-CF20
Edgetek™ NN-50GF/000 PA66-GF50
Edgetek™ PA-45GF/000 BK005 PA*-GF45
Edgetek™ PA-50GF/000 BK004 PA*-GF50
Edgetek™ PA-60GF/000 BK006 PA*-GF60
Edgetek™ PA6-GL30 BK010 PA6-GF30
Edgetek™ PC 15GF/000 NC024 PC-GF15
Edgetek™ PC-000/000 BK102 PC
Edgetek™ PC-000/000 BK710 PC
Edgetek™ PC-10CF/000 NH FR BK033 PC-CF10
Edgetek™ PC-10GF/000 BLK007 PC-GF10
Edgetek™ PC-10GF/000 FR WT088 PC-GF10
Edgetek™ PC-10GF/000 NC063 PC-GF10
Edgetek™ PC-10GF/000 NC088 PC-GF10
Edgetek™ PC-10GF/000 NH FR BK042 PC-GF10
Edgetek™ PC-10GF/000 NH FR NC701 PC-GF10
Edgetek™ PC-15CF-15GF/000 NH FR V0 Black PC-(CF+GF)30
Edgetek™ PC-15CF/000 Black PC-CF15
Edgetek™ PC-15GF/000 BK023 PC-GF15
Edgetek™ PC-15GF/000 NC008 PC-GF15
Edgetek™ PC-20GF/000 FR BK PC-GF20
Edgetek™ PC-20GF/000 FR BLK001 PC-GF20
Edgetek™ PC-20GF/000 FR NATURAL PC-GF20
Edgetek™ PC-20GF/000 MR BK017 PC-GF20
Edgetek™ PC-20GF/000 MR BLACK PC-GF20
Edgetek™ PC-20GF/000 NATURAL PC-GF20
Edgetek™ PC-20GF/000 NC008 PC-GF20
Edgetek™ PC-20GF/000 NH FRV0 BLACK PC-GF20
Edgetek™ PC-20GF/000 NH FRV0 BLK PC-GF20
Edgetek™ PC-30GF/000 BK088 PC-GF30
Edgetek™ PC-40GF/000 BK001 PC-GF40
Edgetek™ PC-40GF/000 BK008 PC-GF40
Edgetek™ PI-30GF/000 PEI-GF30
Edgetek™ PI-30GF/000R BLACK PEI-GF30
Edgetek™ PI-40GF/000 BLACK PEI-GF40
Edgetek™ PK-000/000 EM Natural PEEK
Edgetek™ PK-000/000 Natural PEEK
Edgetek™ PK-10GF/000 PEEK-GF10
Edgetek™ PK-30CF/000 BK PEEK-CF30
Edgetek™ PK-30CF/000 EM BK PEEK-CF30
Edgetek™ PK-30CF/000 FCR BK PEEK-CF30
Edgetek™ PK-30GF/000 BK PEEK-GF30
Edgetek™ PK-30GF/000 EM BK PEEK-GF30
Edgetek™ PK-30GF/000 EM NC PEEK-GF30
Edgetek™ PK-30GF/000 FCR BK PEEK-GF30
Edgetek™ PK-30GF/000 FCR NC PEEK-GF30
Edgetek™ PK-30GF/000 NC PEEK-GF30
Edgetek™ PP 402S GR382 PP
Edgetek™ PS-20GF/000 NATURAL PBT-GF20
Edgetek™ PS-30CF/000 HF UV BLACK PBT-CF30
Edgetek™ PS-50GF/000 NC701 PBT-GF50
Edgetek™ QT-15GF/000 natur SO (PS-SY)-GF15
Edgetek™ QT-20MN/000 natural HI (PS-SY)-(MX+X)
Edgetek™ SF-10CF/000 BK001 PPS-CF10
Edgetek™ SF-30GF/000 BK003 PPS-GF30
Edgetek™ SF-30GF/000 NC005 PPS-GF30
Edgetek™ SF-30GF/000 RS NC PPS-GF30
Edgetek™ SF-40CF/000 PPS-CF40
Edgetek™ SF-40GF/000 NATURAL PPS-GF40
Edgetek™ SF-40GF/000 RS BK001 PPS-GF40
Edgetek™ SF-40GF/000 RS NC PPS-GF40
Edgetek™ SF2-40CF/000 NATURAL PPS-CF40
Edgetek™ UR2-40CF/000 BLACK PUR-CF40
Edgetek™ X AS/018 NC704 ABS
Edgetek™ X ET9800-0030 RS Natural PEEK-GF30
Edgetek™ X PS-154200101 WHITE PBT-GF30
Edgetek™ X4 ET3500-5004 White1 (ASA+PC)
Edgetek™ XP9242701 PPS-(GF+CF)40
Edgetek™ XT X XT 1000 Natural TPC
Edgetek™ XT X XT 1001 Natural TPC
Edgetek sPS® QT-10GB-10MN/000 (PS-SY)-(GB+MD)20
Edgetek sPS® QT-10GF-10MN/000 (PS-SY)-(GF+MD)20
Edgetek sPS® QT-10GF/000 (PS-SY)-GF10
Edgetek sPS® QT-10GF/000 FR (PS-SY)-GF10
Edgetek sPS® QT-15GF-15GB/000 (PS-SY)-(GF+GB)30
Edgetek sPS® QT-20GB/000 (PS-SY)-GB20
Edgetek sPS® QT-20GF/000 (PS-SY)-GF20
Edgetek sPS® QT-22GF/000 FR (PS-SY)-GF22
Edgetek sPS® QT-22MN/000 HI (PS-SY)-MD22
Edgetek sPS® QT-25GF/000 FR (PS-SY)-GF25
Edgetek sPS® QT-30GB/000 (PS-SY)-GB30
Edgetek sPS® QT-30GF/000 FR (PS-SY)-GF30
Edgetek sPS® QT-30GF/000 FR HC (PS-SY)-GF30
Edgetek sPS® QT-40GF/000 (PS-SY)-GF40
Edgetek sPS® QT-40GF/000 FR (PS-SY)-GF40
Edgetek™ AS-20GF/000 ABS-GF20
Edgetek™ CY-1000 UV FR V0 (PC+ABS)
Edgetek™ NI-10GF/000 PA610-GF10
Edgetek™ NN-30GF/000 PA66-GF30
Edgetek™ NN-35MG/000 Black v1.1 PA66
Edgetek™ NN-50GF/000EM L PA66-GF50
Edgetek™ NY-20GF/10GB/000 PA6-(GF+GB)30
Edgetek™ PC-15CF-15GF/000 PC-CF15
Edgetek™ PC-15CF/000 FCR PC-CF15
Edgetek™ PC-20GF/000 PC-GF20
Edgetek™ PE-30GF/000 (PE-HD)-GF30
Edgetek™ PF-05GF/000 FR MR PSU-GF5
Edgetek™ PF-20GF/000 PSU-GF20
Edgetek™ PP-20GF/000 HS PP-GF20
Edgetek™ PP-20GF/XC701 WHITE PP-GF20
Edgetek™ PS-15GF/000 White PBT-GF15
Edgetek™ RA-10GF-10CF/000 HI PPSU-(GF+CF)20
Edgetek™ TR2-10GF/000 NATURAL TPC-GF10
Edgetek™ TR2-30GF/000 NATURAL TPC-GF30
Edgetek™ X TR2-20TA/000 NATURAL TPC-MX
Edgetek™ XT EX3600-0002 UV Black (PC+PBT)
Edgetek™ XT XT-100-BU01-HF (PC+PBT)
Edgetek™ XT XT-100-BU03 Black (PC+PBT)
Edgetek™ XT XT-500-CU00 (PC+PBT)

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.