Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Exceed™ 1018KA - PE - ExxonMobil Chemical

Material Data Center offers the following functions for Exceed™ 1018KA:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Exceed datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics단위시험규격
ASTM 데이터
용융 흐름성, MFI 1 g/10min ASTM D 1238
온도 190 °C -
하중 2.16 kg -
열적 특성단위시험규격
ASTM 데이터
녹는점 119 °C ASTM D 3418
광학 특성단위시험규격
ASTM 데이터
광택도 39 - ASTM D 2457
탁도 18 % ASTM D 1003
기타 특성단위시험규격
밀도 918 kg/m³ ASTM D 792
기계적 성질 (필름) 단위시험규격
ASTM Data
항복강도, 평행 9.65 MPa ASTM D 882
항복강도, 수직 9.65 MPa ASTM D 882
파단시 강도, 평행 54.5 MPa ASTM D 882
파단시 강도, 수직 42.7 MPa ASTM D 882
파단시 신율 , 평행 500 % ASTM D 882
파단시 신율 , 수직 600 % ASTM D 882
압출 유형 blown - -
시편두께 0.0254 mm -
특징
생산 공정
Blown Film Extrusion, 필름 압출
부가물
점착방지제
특별 특성
고충격 또는 고충격 보강
특성
Barrier Properties, Good Drawdown, Thermal Stability, Copolymer, Hexene Copolymer
Certifications
Food contact
응용
포장
지역별 검색
쩐횈쩍횄쩐횈 횇횂횈챵쩐챌 횁철쩔짧
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.