Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of FLEXIRENE® MS 20 A - (PE-LLD) - Versalis S.p.A

Material Data Center offers the following functions for FLEXIRENE® MS 20 A:
unit conversion, PDF datasheet print, comparison with other plastics, flow length calculation, snap fit calculation, beam deflection calculation, cooling time calculation, parameters for material models, CAE Interfaces

Check here, which other Flexirene datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
Linear low density polyethylene with antioxidants.Suitable for injection moulding process.
Flexirene MS 20 A is characterised by otpimum low temperatures properties.

Applications
Detergent containers, stoppers and closures for chemicals, containers for low temperature use.
Its high flowability makes it ideal for masterbatches preparation for LLDPE and LDPE.
Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 부피 - 흐름 속도, MVR 26 cm³/10min ISO 1133
온도 190 °C -
하중 2.16 kg -
용융 밀도 746 kg/m³ -
용융 열전도율 0.39 W/(m K) -
용융 비열용량 2810 J/(kg K) -
이형온도 83 °C -
기계적 특성단위시험규격
ISO 데이터
인장탄성률 150 MPa ISO 527
50%변형하에서의 강도 10 MPa ISO 527
파단시 신율 >50 % ISO 527
쇼어 D 경도 48 - ISO 7619-1
열적 특성단위시험규격
ISO 데이터
녹는점, 10°C/min 113 °C ISO 11357-1/-3
유리 전이 온도, 10 °C/min 101 °C ISO 11357-1/-2
선형 열팽창 계수, 평행 152 E-6/K ISO 11359-1/-2
기타 특성단위시험규격
밀도 921 kg/m³ ISO 1183
도표
점도-변형률 , FLEXIRENE® MS 20 A, (PE-LLD), Versalis
전단-변형률 , FLEXIRENE® MS 20 A, (PE-LLD), Versalis
특징
생산 공정
사출 성형
인도 유형
펠렛 (입자,알갱이)
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬, 짱쨌쨈, 쩐횈쩍횄쩐횈 횇횂횈챵쩐챌 횁철쩔짧, 쨀짼쨘횓 쨔횞 횁횩쩐횙 쩐횈쨍횧쨍짰횆짬, 쨉쩔쩐챌 쨔횞 쩐횈횉횁쨍짰횆짬 짹횢쩔짧
기타 정보
사E성

#2

Typical processing temperature range:

    Melt temperature         160 - 210 °C

    Mold temperature          10-  40  °C

Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.