Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of FORTRON® 4184L4 - PPS-(MD+GF)53 - Celanese

Material Data Center offers the following functions for FORTRON® 4184L4:
unit conversion, PDF datasheet print, comparison with other plastics, application examples, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Fortron datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
Fortron 4184L4 is the strongest and toughest glass/mineral reinforced product available. It offers excellent heat resistance at high loads and good chemical resistance. The electrical properties are excellent and the product is inherently flame-retardant. This product also offers low creep resistance and good rigidity due to the mineral content. Applications made of this grade include electronic components (i.e. bobbins, connectors and solenoid valves).

Flammability @1.6mm nom. thickn.V-0-
Flammability at thickness h (0.75 mm)V-0-
Processing/Physical Characteristics단위시험규격
ISO 데이터
성형 수축률, 평행 0.3 % ISO 294-4, 2577
성형 수축률, 수직 0.6 % ISO 294-4, 2577
용융 비열용량 1600 J/(kg K) -
기계적 특성단위시험규격
ISO 데이터
인장탄성률 16600 MPa ISO 527
파단시 강도 165 MPa ISO 527
파단시 신율 1.4 % ISO 527
챠피 충격 강도 , +23°C 29 kJ/m² ISO 179/1eU
챠피 충격 강도, -30°C 29 kJ/m² ISO 179/1eU
챠피 노치드 충격 강도, +23°C 7 kJ/m² ISO 179/1eA
챠피 노치드 충격 강도, -30°C 7 kJ/m² ISO 179/1eA
열적 특성단위시험규격
ISO 데이터
녹는점, 10°C/min 280 °C ISO 11357-1/-3
유리 전이 온도, 10 °C/min 90 °C ISO 11357-1/-2
하중하에서의 변형온도, 1.80 MPa 270 °C ISO 75-1/-2
하중하에서의 변형온도, 8.00 MPa 215 °C ISO 75-1/-2
선형 열팽창 계수, 평행 24 E-6/K ISO 11359-1/-2
선형 열팽창 계수, 수직 32 E-6/K ISO 11359-1/-2
1.5mm 평균두께에서의 난연성 V-0 class IEC 60695-11-10
테스트 두께 1.5 mm -
두께 H인 제품의 난연성 V-0 class IEC 60695-11-10
테스트 두께 0.8 mm -
전기적 특성단위시험규격
ISO 데이터
상대 유전뮬, 1MHz 4.7 - IEC 62631-2-1
소산 인자, 1MHz 20 E-4 IEC 62631-2-1
부피 저항 >1E13 Ohm*m IEC 62631-3-1
표면 저항 >1E15 Ohm IEC 62631-3-2
전기 압력 27 kV/mm IEC 60243-1
기타 특성단위시험규격
물에서의 흡수성 0.02 % ISO 62와 유사
밀도 1800 kg/m³ ISO 1183
Processing Recommendation Injection Molding단위시험규격
Pre-drying - Temperature 130 - 140 °C -
Pre-drying - Time 3 - 4 h -
용융수지온도 320 - 340 °C -
성형온도 ≥140 °C -
도표
응력-신율 , FORTRON® 4184L4, PPS-(MD+GF)53, Celanese
시컨트탄성율-신율 , FORTRON® 4184L4, PPS-(MD+GF)53, Celanese
특징
생산 공정
사출 성형
인도 유형
펠렛 (입자,알갱이)
부가물
이형제
특별 특성
난연성, 도금가능한, 가시광선 안정성, U.V. 안정성 또는 기후 안정성, 열안정성
특성
Creep Resistance
내화학성에
General Chemical Resistance
응용
전기 및 전자
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬, 짱쨌쨈, 쨀짼쨘횓 쨔횞 횁횩쩐횙 쩐횈쨍횧쨍짰횆짬, 쨉쩔쩐챌 쨔횞 쩐횈횉횁쨍짰횆짬 짹횢쩔짧
기타 정보
사E성
Predrying in a dehumidified air dryer at 130 - 140 degC/3-4 hours is recommended.
On injection molding machines with 15-25 D long three-section screws, as are usual in the trade, the FORTRON is processable. A shut-off nozzle is preferred to a free-flow nozzle.

Melt temperature 320-340 degC
Mold wall temperature at least 140 degC

A medium injection rate is normally preferred. All mold cavities must be effectively vented.
Tool temperature of at least 135 degC is recommended for parts to achieve maximum crystallizable potential.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.